Modified polypropylene for automobile bumper and preparation method of modified polypropylene
A technology of automobile bumper and polypropylene, which is applied in the field of modified polypropylene for automobile bumper and its preparation, which can solve the problem of the improvement of scratch resistance, the decline of physical properties of aging resistance and corrosion resistance, and the difficulty of taking into account various Performance and other issues, to achieve the effect of improving rigidity, toughness and balance, and broad application prospects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] A modified polypropylene for automobile bumpers, which is made of the following raw materials in parts by weight: 40 parts of polypropylene, 30 parts of EPDM rubber, 0.4 parts of 2,8-di-tert-butyl-4-methylphenol, 0.4 parts of phosphate ester, 2 parts of zinc oxide, 2 parts of copper fiber, 1 part of organic fiber, 22 parts of talcum powder, 1 part of zinc aluminum oxide, 0.2 part of coupling agent, 0.5 part of colorant, 0.8 part of SN, 0.5 part of vulcanizing agent , Accelerator 0.4 part.
[0019] The above-mentioned preparation method of modified polypropylene for automobile bumper comprises the following steps: (1) Weighing each raw material according to the weight part, for later use; (2) Adding EPDM rubber into an open mill and masticating for 15 minutes , the machine temperature is less than 35°C, the roller distance is 0.8mm, then add zinc oxide, copper fiber, organic fiber, talcum powder, zinc aluminum oxide, coupling agent, SN, vulcanizing agent, accelerator, co...
Embodiment 2
[0021] A modified polypropylene for automobile bumper, which is made of the following raw materials in parts by weight: 45 parts of polypropylene, 54 parts of EPDM rubber, 0.5 part of 2,8-di-tert-butyl-4-methylphenol, 0.6 parts of phosphate ester, 2.5 parts of zinc oxide, 2.5 parts of copper fiber, 1.2 parts of organic fiber, 24.75 parts of talcum powder, 1.2 parts of zinc aluminum oxide, 0.25 parts of coupling agent, 0.7 parts of coloring agent, 1 part of SN, 0.7 parts of vulcanizing agent , Accelerator 0.5 part.
[0022] The above-mentioned preparation method of modified polypropylene for automobile bumper comprises the following steps: (1) Weighing each raw material according to the weight part, for later use; (2) Adding EPDM rubber into an open mill and masticating for 17 minutes , the machine temperature is less than 35°C, the roller distance is 1mm, then add zinc oxide, copper fiber, organic fiber, talcum powder, zinc aluminum oxide, coupling agent, SN, vulcanizing agent...
Embodiment 3
[0024]A modified polypropylene for automobile bumpers, which is made of the following raw materials in parts by weight: 50 parts of polypropylene, 66.7 parts of EPDM rubber, 0.6 parts of 2,8-di-tert-butyl-4-methylphenol, 0.8 parts of phosphate ester, 3 parts of zinc oxide, 4 parts of copper fiber, 2 parts of organic fiber, 29 parts of talcum powder, 2 parts of zinc aluminum oxide, 0.3 part of coupling agent, 1 part of colorant, 1.2 parts of SN, 0.8 part of vulcanizing agent , Accelerator 0.6 part.
[0025] The above-mentioned preparation method of modified polypropylene for automobile bumper comprises the following steps: (1) Weighing each raw material according to the weight part, and setting it aside; (2) Adding EPDM rubber into an open mill and masticating for 20 minutes , the machine temperature is less than 35°C, the roller distance is 1.2mm, then add zinc oxide, copper fiber, organic fiber, talcum powder, zinc aluminum oxide, coupling agent, SN, vulcanizing agent, accele...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com