[0030] The present embodiment provides a kind of wood coloring method, comprising:
[0031] (1) Sterilization: sterilize the wood under an ultraviolet lamp;
[0032] (2) soaking: dry the wood after the first soaking in the dye solution;
[0033] (3) Cooking: dry the wood after the first cooking in the dye solution;
[0034] (4) Soaking: dry the wood after the second soaking in the dye solution;
[0035] (5) Cooking: dry the wood after the second cooking in the dye solution;
[0036] (6) Dyeing: the dye solution is applied to the surface of the wood and then dried;
[0037] (7) Baking: the wood obtained in step (6) is wrapped with peat and then dried to obtain colored wood.
[0038] The initial density of wood is 0.4g / cm 3 .
[0039] In step (1), the sterilization time is 30min.
[0040] In step (2), the temperature of the dye solution during the first soaking is 25° C., the soaking time is 30 minutes, and the wood is completely submerged in the dye solution during soaki...
Embodiment 2
[0049] The present embodiment provides a kind of wood coloring method, comprising:
[0050] (1) Sterilization: sterilize the wood under an ultraviolet lamp;
[0051] (2) soaking: dry the wood after the first soaking in the dye solution;
[0052] (3) Cooking: dry the wood after the first cooking in the dye solution;
[0053] (4) Soaking: dry the wood after the second soaking in the dye solution;
[0054] (5) Cooking: dry the wood after the second cooking in the dye solution;
[0055] (6) Dyeing: the dye solution is applied to the surface of the wood and then dried;
[0056] (7) Baking: the wood obtained in step (6) is wrapped with peat and then dried to obtain colored wood.
[0057] The initial density of wood is 0.55g / cm 3 .
[0058] In step (1), the sterilization time is 40min.
[0059] In step (2), the temperature of the dye solution during the first soaking is 30° C., the soaking time is 20 minutes, and the wood is completely submerged in the dye solution during soak...
Embodiment 3
[0068] The present embodiment provides a kind of wood coloring method, comprising:
[0069] (1) Sterilization: sterilize the wood under an ultraviolet lamp;
[0070] (2) soaking: dry the wood after the first soaking in the dye solution;
[0071] (3) Cooking: dry the wood after the first cooking in the dye solution;
[0072] (4) Soaking: dry the wood after the second soaking in the dye solution;
[0073] (5) Cooking: dry the wood after the second cooking in the dye solution;
[0074] (6) Dyeing: the dye solution is applied to the surface of the wood and then dried;
[0075] (7) Baking: the wood obtained in step (6) is wrapped with peat and then dried to obtain colored wood.
[0076] The initial density of wood is 0.5g / cm 3 .
[0077] In step (1), the sterilization time is 50min.
[0078] In step (2), the temperature of the dye solution during the first soaking is 25° C., the soaking time is 30 minutes, and the wood is completely submerged in the dye solution during soaki...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com