Embodiment 1
[0024] A kind of formula of cabinet mat, comprises following components and parts by weight thereof:
[0025] Phase A components: 10 parts of thermoplastic rubber, 16 parts of thermoplastic elastomer, 5 parts of liquid paraffin, 13 parts of microcrystalline wax, 3 parts of color masterbatch;
[0026] Phase B components: 60 parts of impact-resistant polystyrene, 2 parts of color masterbatch.
[0027] The method for preparing the cupboard mat by utilizing the formula of the cupboard mat may further comprise the steps:
[0028] S1, batching: batching is carried out according to the weight part of each component, obtains A phase component and B phase component respectively;
[0029] S2. Drying treatment: put the components of phase A into an oven, control the temperature at 80°C, and dry and dehumidify for 2 hours;
[0030] S3. Stirring and mixing: put the A phase component and the B phase component into different agitators respectively, control the stirring speed of the two agi...
Embodiment 2
[0037] A kind of formula of cabinet mat, comprises following components and parts by weight thereof:
[0038] Phase A components: 15 parts of thermoplastic rubber, 12 parts of thermoplastic elastomer, 8 parts of liquid paraffin, 10 parts of microcrystalline wax, 3.5 parts of color masterbatch;
[0039] Phase B components: 55 parts of impact-resistant polystyrene, 3 parts of color masterbatch.
[0040] The method for preparing the cupboard mat by utilizing the formula of the cupboard mat may further comprise the steps:
[0041] S1, batching: batching is carried out according to the weight part of each component, obtains A phase component and B phase component respectively;
[0042] S2. Drying treatment: Put the components of phase A into an oven, control the temperature at 70°C, and dry and dehumidify for 2.5 hours;
[0043] S3. Stirring and mixing: Put the A phase component and the B phase component into different agitators respectively, control the stirring speed of the two...
Embodiment 3
[0050] A kind of formula of cabinet mat, comprises following components and parts by weight thereof:
[0051] Phase A components: 20 parts of thermoplastic rubber, 8 parts of thermoplastic elastomer, 10 parts of liquid paraffin, 6 parts of microcrystalline wax, 4 parts of color masterbatch;
[0052] Phase B components: 50 parts of impact-resistant polystyrene, 4 parts of color masterbatch.
[0053] The method for preparing the cupboard mat by utilizing the formula of the cupboard mat may further comprise the steps:
[0054] S1, batching: batching is carried out according to the weight part of each component, obtains A phase component and B phase component respectively;
[0055] S2. Drying treatment: put the components of phase A into an oven, control the temperature at 60°C, and dry and dehumidify for 3 hours;
[0056] S3. Stirring and mixing: Put the A phase component and the B phase component into different agitators respectively, control the stirring speed of the two agit...