Rock diffusion coefficient measuring device and method
A technology of diffusion coefficient and measurement device, applied in measurement device, diffusion analysis, instrument and other directions, can solve the problems of not considering the pressure difference on both sides of the rock sample, poor reliability of measurement results, low test efficiency, etc., to shorten the sealing installation time, Simple structure and the effect of reducing production cost
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0043] A specific embodiment of the present invention, such as figure 1 As shown, a rock diffusion coefficient measurement device is disclosed, including a tracer solution pipeline 2, a blank solution pipeline 4, a peristaltic pump 3 and a pressure regulating device, wherein the peristaltic pump 3 is used to drive the tracer solution pipeline 2 and The solution flow in the blank solution pipeline 4, the pressure regulating device is used to regulate the pressure of the tracer solution pipeline 2 and the blank solution pipeline 4; the tracer solution pipeline 2 includes the tracer solution bottle 1 and the tracer solution bottle 1 The connected tracer solution chamber 6, the blank solution pipeline 4 includes a blank solution bottle 5 and a blank solution chamber 8 connected to the blank solution bottle 5, the tracer solution chamber 6 and the blank solution chamber 8 are connected to the rock sample packaging tube 7 and the The rock sample 12 is sealed and connected; the liqui...
Embodiment 2
[0055] This embodiment discloses a rock diffusion coefficient measurement method, specifically using the rock diffusion coefficient measurement device in Embodiment 1 for measurement, including the following steps:
[0056]Step 1: Preprocessing the collected rock samples to obtain the rock samples to be tested. The collected rock samples are cut into cylinders along the vertical bedding direction. Preferably, the rock samples have a diameter of 1-2 cm and a height of 1.5-2 cm. Put the cylindrical rock sample into a mold with an inner diameter of 2.5 cm, add liquid epoxy resin containing a curing agent into the annular space between the rock sample and the inner wall of the mold, and the liquid epoxy resin surrounds the rock sample and embeds it. The liquid epoxy resin can be cured at normal temperature, forming epoxy resin layer 13 on the outer periphery of the rock sample, and the epoxy resin layer 13 after curing is tightly and fixedly connected with the outer peripheral sur...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com