Cosmetic composite, and preparation method and spray of cosmetic composite
A technology of cosmetic composition and extract, which is applied in the field of cosmetic composition, its preparation and spraying, can solve the problems of skin barrier damage and allergy, and achieve the effect of repairing the skin barrier, mild and non-irritating skin, and good stability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0047] The present invention provides a kind of preparation method of allergy-relieving spray, and its formula composition according to weight percentage is:
[0048]
[0049] Preferably, in the soothing spray provided by the present invention, the formula composition according to the weight percentage is:
[0050]
[0051] More preferably, in the soothing spray provided by the present invention, the formula composition according to the weight percentage is:
[0052]
[0053] The preparation method of Shumin spray is carried out according to the following steps after weighing the above-mentioned raw materials according to the weight ratio:
[0054] 1) Add the purified water in phase A into the beaker, heat to 80.5-84.5°C, and keep it warm for 5 minutes;
[0055] 2) Then cool while stirring, when the temperature drops to 50.5-54.5°C, add the pre-dispersed B phase formula, stir well until completely dissolved;
[0056] 3) Then cool while stirring, and when the tempera...
Embodiment 1-3
[0060] Embodiment 1-3: the preparation of spray of the present invention
[0061] Preparation of phase B materials: Add the small molecule sodium hyaluronate and Demisol in phase B into the beaker containing 1,3-butanediol in phase B, and then stir until the dispersion is not agglomerated.
[0062] Preparation of phase D material: Add the arginine in phase D into a beaker containing purified water of phase D, and stir until it dissolves into a transparent liquid.
[0063] 1) Add the purified water in phase A into the beaker, heat to 80.5-84.5°C, and keep it warm for 5 minutes;
[0064] 2) Then cool while stirring, when 1) the temperature drops to 50.5-54.5°C, add the pre-dispersed B-phase formula, stir well until completely dissolved;
[0065] 3) Then cool down while stirring, and when the temperature in 2) drops to 30-33°C, add the phase C material and the pre-dissolved phase D formula in sequence, and continue to stir evenly after adding the materials;
[0066] 4) Stop sti...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com