Sulfur-containing compound peculiar smell eliminating agent as well as preparation method and application thereof
A technology of odor eliminators and compounds, applied in the field of odor eliminators and their preparation, to achieve the effect of reducing odor nuisance and improving satisfaction
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0031] At normal temperature, 5 kg of 100 mesh powdered activated carbon was soaked in 50 kg of potassium permanganate saturated aqueous solution for 2.5 hours by impregnation method; filtered through 100 mesh and dried at 90°C, 100 mesh of potassium permanganate modified powdered activated carbon was obtained for subsequent use.
[0032] Soak the 200 mesh zeolite of 2kg in 20kg potassium permanganate saturated aqueous solution for 2.5 hours; filter through 140 mesh and dry at 100°C to obtain 200 mesh potassium permanganate modified zeolite for subsequent use;
[0033] The 170 order ferric chloride of described potassium permanganate modified powder activated carbon, potassium permanganate modified zeolite and 30kg is carried out solid-phase mixing, rotating speed 50rmp, obtain described odor eliminating agent after stirring for 2 hours;
[0034] At the site of a soil restoration project in a certain pesticide-contaminated site, select the larger construction exposure surface o...
Embodiment 2
[0036] At normal temperature, 2.3kg of 200 mesh powdered activated carbon was immersed in 70kg potassium permanganate saturated aqueous solution for 3 hours by impregnation method; filtered through 200 mesh and dried at 80°C, 100 mesh potassium permanganate modified powdered activated carbon was obtained for subsequent use.
[0037] Soak 0.7kg of 100-mesh zeolite in 20kg of potassium permanganate saturated aqueous solution for 3 hours; filter through 170-mesh and dry at 95°C to obtain 200-mesh potassium permanganate modified zeolite for use;
[0038] The 100 order ferric chloride of described potassium permanganate modified powder activated carbon, potassium permanganate modified zeolite and 10kg is carried out solid-phase mixing, rotating speed 200rmp, obtain described peculiar smell eliminating agent after stirring for 1 hour;
[0039] On the site of a certain pesticide-contaminated site soil remediation project, select the relatively large construction exposure surface of th...
Embodiment 3
[0041] At normal temperature, soak 2.5kg of 140 mesh powdered activated carbon in 50kg potassium permanganate saturated aqueous solution for 2 hours by impregnation method; filter through 120 mesh and dry at 85°C to obtain 170 mesh potassium permanganate modified powdered activated carbon for subsequent use.
[0042] Soak the 200 mesh zeolite of 2kg in 30kg potassium permanganate saturated aqueous solution for 2 hours; Filter through 200 mesh and dry at 80°C to obtain 200 mesh potassium permanganate modified zeolite for subsequent use;
[0043] The 100 order ferric chloride of described potassium permanganate modified powder activated carbon, potassium permanganate modified zeolite and 20kg is carried out solid-phase mixing, rotating speed 150rmp, obtain described peculiar smell eliminating agent after stirring for 1.5 hours;
[0044] At the site of a soil restoration project in a certain pesticide-contaminated site, select the larger construction exposed surface of the peculia...
PUM
Property | Measurement | Unit |
---|---|---|
particle size (mesh) | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com