Zirconium-containing nano slow-release anti-ulcer fertilizer and preparation method thereof
A nano-sustained release and canker disease technology, which is applied in the direction of organic fertilizers, inorganic fertilizers, ammonium salt fertilizers, etc., can solve problems such as excessive copper ion content and environmental pollution, and achieve improved immunity, rich nutrition, and resistance to dipping and harm Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0051] A zirconium-containing nano slow-release anti-canker fertilizer, in parts by weight, said fertilizer includes 50 parts of zirconium-containing nano-earth material, 5 parts of zeolite powder, 0.005 part of copper sulfate, 0.001 part of ammonium molybdate, and 0.1 part of zinc sulfate , 1.5 parts of vitamin C, 16 parts of organic matter, 0.005 parts of Bacillus subtilis, 5 parts of urea, 15 parts of monoammonium phosphate, 15 parts of potassium sulfate, and 15 parts of water.
[0052] The preparation method of the zirconium-containing nano-earth material comprises the following steps:
[0053] (1) In parts by weight, 100 parts of natural nano-earth materials are dried, crushed and sieved through 300 meshes, and set aside;
[0054] (2) Add 0.01 part of zirconium sulfate to 200 parts of water, stir and dissolve, and heat to 45° C., add 10 parts of citric acid, stir at constant temperature for 45 minutes, add the natural nano-earth material powder obtained in step (1), and s...
Embodiment 2
[0067] A zirconium-containing nano slow-release anti-canker disease fertilizer, in parts by weight, said fertilizer includes 55 parts of zirconium-containing nano-earth materials, 10 parts of zeolite powder, 0.007 parts of copper sulfate, 0.003 parts of ammonium molybdate, and 0.15 parts of zinc sulfate , 2.2 parts of vitamin C, 18 parts of organic matter, 0.007 parts of Bacillus subtilis, 7 parts of urea, 18 parts of monoammonium phosphate, 18 parts of potassium sulfate, and 18 parts of water.
[0068] The preparation method of the zirconium-containing nano-earth material comprises the following steps:
[0069] (1) In parts by weight, 110 parts of natural nano-earth materials are dried, pulverized and sieved with 325 mesh, and set aside;
[0070] (2) Add 0.015 parts of zirconium sulfate to 250 parts of water, stir and dissolve, and heat to 50° C., add 15 parts of citric acid, stir at constant temperature for 36 minutes, add the natural nano-earth material powder obtained in s...
Embodiment 3
[0083] A zirconium-containing nano slow-release anti-canker disease fertilizer, in parts by weight, said fertilizer includes 60 parts of zirconium-containing nano-earth materials, 15 parts of zeolite powder, 0.01 part of copper sulfate, 0.005 part of ammonium molybdate, and 0.2 part of zinc sulfate , 3.0 parts of vitamin C, 20 parts of organic matter, 0.01 parts of Bacillus subtilis, 10 parts of urea, 20 parts of monoammonium phosphate, 20 parts of potassium sulfate, and 20 parts of water.
[0084] The preparation method of the zirconium-containing nano-earth material comprises the following steps:
[0085] (1) In parts by weight, 120 parts of natural nano-earth materials are dried, pulverized and sieved with 350 meshes for subsequent use;
[0086] (2) Add 0.02 parts of zirconium sulfate to 300 parts of water, stir and dissolve, and heat to 55° C., add 20 parts of citric acid, stir at constant temperature for 30 minutes, add the natural nano-earth material powder obtained in s...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com