High-viscosity fog seal material for pre-maintenance of drainage asphalt pavement and preparation method thereof
A technology of fog sealing layer material and drainage asphalt, applied in the direction of asphalt coating, coating, etc., can solve the problems of easy hardening and brittle temperature sensitivity, easy flow, restricting the application of asphalt materials, etc., to protect the pavement structure and prolong the use. Longevity, effect of preventing further aging
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] The high-viscosity mist sealant material for drainage asphalt pavement pre-maintenance of the present invention is composed of A component and B component, the mass ratio of the A component to the B component is 7:3, and the A component is composed of a matrix The mixture of asphalt and SBS modifier constitutes, the mass ratio of base asphalt and SBS modifier is 63:7, and the B component cyclohexane, kerosene, expanded vermiculite and cetyltrimethylammonium bromide according to The mass ratio is 3:20:3:4.
[0026] The preparation method of the high-viscosity mist sealant material for the pre-maintenance of the above-mentioned drainage asphalt pavement is carried out according to the following steps:
[0027] Step 1, preparation of component A: put base asphalt in an oven at 130°C, heat for 30 minutes to melt and dehydrate, add SBS modifier to the asphalt, shear, stir evenly and cool down to below 50°C;
[0028] Step 2, preparing component B: adding cyclohexane, expande...
Embodiment 2
[0031] The high-viscosity mist sealant material for drainage asphalt pavement pre-maintenance of the present invention is composed of A component and B component, the mass ratio of the A component to the B component is 7:3, and the A component is composed of a matrix The mixture of asphalt and SBS modifier constitutes, the mass ratio of base asphalt and SBS modifier is 65:5, and the B component cyclohexane, kerosene, expanded vermiculite and cetyltrimethylammonium bromide according to The mass ratio is 2:20:3:5.
[0032] The preparation method of the high-viscosity mist sealant material for the pre-maintenance of the above-mentioned drainage asphalt pavement is carried out according to the following steps:
[0033] Step 1, prepare component A: put base asphalt in an oven at 140°C, heat for 40 minutes to melt and dehydrate, add SBS modifier to the asphalt, shear, stir evenly and cool down to below 50°C;
[0034] Step 2, preparing component B: adding cyclohexane, expanded vermi...