A surfactant and fatty acid technology, which is applied in the mixed system containing fatty acid surfactant and its preparation field, can solve the problems of easy crystallization and low concentration of fatty acid, etc., and achieve the effect of easy popularization and application, simple formula and preparation method
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0018] The method for preparing a mixed system containing a fatty acid type surfactant provided by the invention comprises mixing a long-chain fatty acid with 11-14 carbon atoms, 3,3'-iminobis(N,N-dimethylpropylamine) and water Mix until the solid is dissolved, wherein the molar ratio between the long-chain fatty acid and 3,3'-iminobis(N,N-dimethylpropylamine) is 295-305:100, preferably 3:1.
[0019] In the present invention, by combining specific long-chain fatty acids and amines, the use concentration of long-chain fatty acids can be increased, therefore, the content of the long-chain fatty acids can be as high as 50% by weight, preferably, based on the total weight of the mixed system As a basis, the content of the long-chain fatty acid is 0.1-50% by weight.
[0020] According to the present invention, the long-chain fatty acid is a fatty acid with 11-14 carbon atoms, preferably a straight-chain fatty acid, including saturated straight-chain fatty acid and / or unsaturated st...
Embodiment 1-21
[0031]According to the dosage shown in Table 1, weigh the long-chain fatty acid and IBDPA and put them in the sample bottle, then add deionized water; after airtight, the mixing method is constant temperature or repeated temperature rise and fall, see the mixing method column "constant temperature" or " repeated heating and cooling". The constant temperature method is to heat the sample to a certain temperature (see Table 1 "Temperature" column for details) and keep the temperature for a certain period of time (see Table 1 "Constant Temperature Time" column for details) until all the solids are dissolved to obtain a mixed system sample; Heating to a certain temperature (see Table 1 "Temperature" column for details) and constant temperature for a certain period of time (see Table 1 "Constant Temperature Time" column for details), then cool to about 0°C and keep the temperature for 10 minutes, and repeat the temperature rise and fall several times (see Table 1 for the number of r...