A detection method for the corrosion resistance of lithium-ion battery uv glue to electrolyte
A lithium-ion battery and detection method technology, applied in the direction of weather resistance/light resistance/corrosion resistance, using stable tension/pressure testing material strength, measuring devices, etc., to achieve the effect of improving accuracy
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0026] A method for detecting the corrosion resistance of lithium-ion battery UV glue to electrolyte, comprising the following steps:
[0027] S1. Weld the empty aluminum shell with the cover plate provided with the liquid injection port and the explosion-proof valve to obtain the shell, and pass nitrogen gas into the inside of the shell for air-tightness testing to ensure that the air-tightness of the shell is qualified;
[0028] S2. Place the airtight qualified housing in a liquid injection room with a dew point ≤ -40°C, inject 10 mg of electrolyte solution containing lithium hexafluorophosphate through the liquid injection port, and clean the residual electrolyte in the liquid injection port with alcohol;
[0029] S3, using UV glue to seal the liquid injection port by dispensing;
[0030] S4. Use a mercury lamp to cure the UV glue at the liquid injection port for 20 seconds, and then let it stand at room temperature for 12 hours;
[0031] S5. Invert the case treated in ste...
Embodiment 2
[0035] A method for detecting the corrosion resistance of lithium-ion battery UV glue to electrolyte, comprising the following steps:
[0036] S1. Weld the empty aluminum shell with the cover plate provided with the liquid injection port and the explosion-proof valve to obtain the shell, and pass nitrogen gas into the inside of the shell for air-tightness testing to ensure that the air-tightness of the shell is qualified;
[0037] S2. Place the airtight qualified housing in a liquid injection room with a dew point ≤ -40°C, inject 10 mg of electrolyte solution containing lithium hexafluorophosphate through the liquid injection port, and clean the residual electrolyte in the liquid injection port with alcohol;
[0038] S3, using UV glue to seal the liquid injection port by dispensing;
[0039] S4. Use LED lamps to cure the UV glue at the liquid injection port for 10 seconds, and then let it stand at room temperature for 12 hours;
[0040] S5. Invert the case treated in step S4 ...