A supported catalyst and catalyst technology, applied in the direction of molecular sieve catalysts, physical/chemical process catalysts, chemical instruments and methods, etc., can solve the problems of high reaction temperature, low yield of aromatics, low methane conversion rate, etc., to achieve easy operation, The effect of simple preparation method
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0024] CuSO containing 0.015g Cu element 4 .5H 2 O, completely dissolved in 5g of deionized water, added ammonium molybdate containing 0.15g of Mo element, after mixing, impregnated the solution on 3g of HZSM-5 molecular sieve carrier, the atomic ratio of Si / Al in HZSM-5 = 15,60 Stir at ℃ for 5h, stir at 80℃ and dry directly, and then bake at 400℃ for 4h to prepare supported CuO-MoO Y / HZSM-5 molecular sieve catalyst, wherein, element A is Cu element, and the content of HZSM-5 molecular sieve is 100 parts by weight, the content of Cu element is 0.5 parts by weight, and the content of Mo element is 5 parts by weight.
Embodiment 2
[0026] Ce(NO 3 ) 3 .6H 2 O was completely dissolved in 10g of deionized water, and ammonium molybdate containing 0.06g of Mo was added. After mixing, the solution was impregnated on 3g of HZSM-5 molecular sieve carrier. The atomic ratio of Si / Al in HZSM-5 was 38,80 Stir for 8 h at 100 °C, dry directly at 100 °C, and then roast at 550 °C for 6 h to prepare the supported Ce 2 o 3 -MoO Y / HZSM-5 molecular sieve catalyst, wherein, element A is Ce element, the content of Ce element is 1 part by weight, and the content of Mo element is 2 parts by weight based on 100 parts by weight of HZSM-5 molecular sieve.
Embodiment 3
[0028] Cr(NO) containing 0.09g Cr element 3 ) 3 .9H 2 Dissolve O completely in 50g deionized water, add ammonium molybdate containing 0.015g Mo element, mix well and impregnate the solution on 3g HZSM-5 molecular sieve carrier, Si / Al atomic ratio in HZSM-5=60, 100℃ Stirring for 10 hours at 120°C, drying directly at 120°C, and then roasting at 650°C for 8 hours to prepare the supported Cr 2 o 3 -MoO Y / HZSM-5 molecular sieve catalyst, wherein, element A is Cr element, the content of Cr element is 3 parts by weight, and the content of Mo element is 0.5 part by weight based on 100 parts by weight of HZSM-5 molecular sieve.