Examples
Embodiment 1
[0011] The environment-friendly water-based sight-seeing agent (i.e. wood brown eye filler) of the present invention is based on degreasing and degumming bone meal, methanol, hydroxymethyl cellulose diluted with water, XG-037 water-based defoamer, and XG-3 high-efficiency preservative , water, XG-202 polyurethane rheology modifier, and XG-301 general-purpose wetting agent are mixed as components. Wherein the weight ratio of each component is: 700 grams of defatted and degummed bone powder, 520 grams of methanol, 250 grams of hydroxymethyl cellulose diluted with water (238.1 grams of water, 11.9 grams of hydroxymethyl cellulose), XG-037 water-based disinfectant 10 drops of foaming agent (about 2 grams), 60 grams of XG-3 high-efficiency preservative, 120 grams of water (softened water is optional), 2 grams of XG-202 polyurethane rheology modifier, 10 grams of XG-301 general-purpose wetting agent gram.
[0012] The above degreased and degummed bone meal can be purchased from Gui...
Embodiment 2
[0029] The environment-friendly water-based sighting agent of the present invention is made of degreasing degummed bone meal, methanol, hydroxymethyl cellulose diluted with water, XG-037 water-based defoamer, XG-3 high-efficiency preservative, demineralized water, and XG-202 polyurethane fluid Modification modifier and XG-301 general-purpose wetting agent are made by mixing components (that is, the sighting agent is composed of the above eight components). Wherein the weight ratio of each component is: 500 grams (or 750 grams or 1000 grams) of defatted degummed bone powder, 550 grams (or 500 grams or 600 grams) of methanol, 200 grams (or 300 grams) of hydroxymethylcellulose diluted with water gram or 400 grams, the weight ratio of water and hydroxymethyl cellulose is 20:1), 1-5 drops of XG-037 water-based defoamer (about 0.2-1 gram), 100 grams of XG-3 high-efficiency preservative ( Or 50 grams or 75 grams), demineralized water 150 grams (or 100 grams or 200 grams), XG-202 poly...
PUM