N3 pigment composition and color block of the composition
A composition and pigment technology, applied in the direction of pigment slurry, pigment-containing coating, color measuring device, etc., can solve the problem of inability to precisely control, and achieve the effect of strong practical value, refined production process, and good ratio reproducibility
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0024] Weigh 16.13 grams of PY42, 3.78 grams of PR101, 11.37 grams of PBK7, 21.34 grams of PW6, and 1000 grams of CSC-C base material by weight. Mix the above-mentioned raw materials, and then apply the mixed composition evenly and evenly on the coated paper by mechanical coating method under the environmental conditions of relative humidity of 50%±5% and room temperature of 23±2°C. The wet film thickness of the coating is 250 μm, then it is dried in a precision oven at 50 ± 2 °C for 3 to 4 hours to a constant weight, taken out, and cooled to room temperature to obtain a physical color block.
Embodiment 2
[0026] Weigh 15.13 grams of PY42, 3.68 grams of PR101, 10.37 grams of PBK7, 20.34 grams of PW6, and 1000 grams of CSC-C base material by weight. The production process is the same as that of Example 1.
Embodiment 3
[0028] Weigh 17.13 grams of PY42, 3.88 grams of PR101, 12.37 grams of PBK7, 22.34 grams of PW6, and 1005 grams of CSC-C base material by weight. The production process is the same as that of Example 1.
PUM
| Property | Measurement | Unit |
|---|---|---|
| particle size | aaaaa | aaaaa |
| minimum film forming temperature | aaaaa | aaaaa |
| glass transition temperature | aaaaa | aaaaa |