Problems solved by technology
Method used
Examples
Embodiment 1
[0006] Embodiment 1: A kind of preparation technology of water-soluble environment-friendly nano paint, with 150 parts of water, 25 parts of ethylene glycol, 52 parts of AMP-9, 1 part of wetting agent, 10 parts of dispersant, 0.5 part of defoamer, nano 150 parts of titanium dioxide, 180 parts of lithopone, 100 parts of nano-calcium, 20 parts of talcum powder, 25 parts of aluminum silicate, put into the disperser and disperse for 10 minutes.
Embodiment 2
[0007] Embodiment 2: A kind of preparation technology of water-soluble environment-friendly nano-coating, with 190 parts of nano-emulsions, 6 parts of alcohol ester-12, 4 parts of diethylene glycol butyl ethers, 85 parts of water, 0.5 parts of defoamers, 0.1 parts of nano-bactericides 3 parts, 7 parts of ASE-60, 16 parts of D-105, 2 parts of preservative, put into the disperser to disperse at low speed, and then pump into the sand mill for sand grinding to produce the finished product.
PUM

Abstract
Description
Claims
Application Information

- R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com