Rolling method in chemical fiber high-stretch yarn adding process
A process and chemical fiber technology, which is applied in the winding field of chemical fiber texturizing process, can solve the problems of high labor intensity of operators, reduction of spindle speed, low processing efficiency, etc., to reduce labor intensity, increase spinning speed and production efficiency Improved effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment Construction
[0016] Specific embodiments of the present invention will be described in detail below in conjunction with the accompanying drawings.
[0017] see figure 2 Shown, the winding method in the chemical fiber texturing process of the present invention, its steps are:
[0018] 1) Spin-up: the high elastic yarn 18 formed after heating, cooling, false twisting and drafting is led out by the middle roller 6, and the high elastic yarn 18 is sucked by the first negative pressure suction device, that is, the upper suction gun 12 live, and then by moving the upper thread suction gun 12, the high elastic thread 18 is pulled to the vicinity of the second negative pressure thread suction device placed on the ring 8, that is, the lower thread suction gun 13, so that the high elastic thread 18 transitions to the first The second negative pressure wire suction device is the lower wire suction gun 13, and then the high elastic wire 18 is sent into the steel wire hook 9 on the steel ring 8;
[...