A kind of preparation method of wallpaper base paper
A wallpaper and base paper technology, applied in the pulp beating method, paper, papermaking, etc., can solve the problems of poor dry and wet strength, unclear pattern displacement, difficult construction, etc., and achieve the effect of increasing strength performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0008] A production method of environment-friendly wallpaper base paper, which is characterized in that it is made of the following raw materials in parts by mass: bamboo fiber 40, wood pulp fiber 45, polyester fiber 25, sodium carboxymethyl cellulose 6, nano-bamboo carbon fiber 8, negative ion powder 5. The production steps are as follows: 1) After mixing bamboo fiber and wood pulp fiber, add water with a mass of 100 times, beat with a beater, and control the beating degree at 40-60 ° SR, wherein the bamboo fiber and wood pulp fiber After mixing, add nano-carbon fiber and nano-far-infrared negative ion powder into the mixed pulp evenly. Nano-carbon fiber is added 1-2 hours after the beating starts. After adding nano-carbon fiber, continue beating for 0.5-1 hour and add nano-far-infrared negative ions 2) adding 100 times of water to the polyester fiber and beating with a beater for 20 to 40 minutes to obtain a polyester fiber pulp; 3) mixing the bamboo fiber in the above steps ...
Embodiment 2
[0010] A production method of environment-friendly wallpaper base paper, which is characterized in that it is made of the following raw materials in parts by mass: bamboo fiber 35, wood pulp fiber 30, polyester fiber 15, sodium carboxymethyl cellulose 2, nano-bamboo carbon fiber 2, negative ion powder 2. The production steps are as follows: 1) After mixing bamboo fiber and wood pulp fiber, add water with a mass of 100 times, beat with a beater, and control the beating degree at 40-60°SR, wherein after mixing bamboo fiber and wood pulp fiber , adding nano-carbon fiber and nano far-infrared negative ion powder to the mixed pulp evenly, nano-carbon fiber is added 1 to 2 hours after the beating starts, after adding nano-carbon fiber, continue beating for 0.5-1 hour to add nano-far-infrared negative ion powder, Promptly make the mixed pulp of bamboo fiber and wood pulp fiber; 2) add 100 times of water to the polyester fiber, and beat for 20 to 40 minutes with a beater to make polye...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com