Examples
preparation example Construction
[0044] (1) Preparation of solution A: Add water to the container, slowly add carboxymethyl guar gum while stirring with a pump or stirrer, and then add surfactant, clay stabilizer and fungicide respectively , Continue to circulate or stir for 30 minutes after adding the temperature-resistant enhancer, so that the liquid can be fully mixed to form solution A.
[0045] (2) During fracturing construction, while pumping solution A, mix solution A and L-11 cross-linking agent with the volume of solution A:JL-11 cross-linking agent=100:0.15~100:.025 Mixed to form fracturing fluid. the
Embodiment 1
[0047] First, the following materials are proportioned according to parts by weight:
[0048] 96.15 parts of water
[0049] Carboxymethyl guar gum 0.25 parts
[0050] Organic zirconium crosslinking agent 0.15 parts
[0051] Hydrocarbon emulsifier 0.30 parts
[0052] Trimethylhydroxypropyl quaternary ammonium salt clay stabilizer 0.20 parts
[0053] Dodecyl dimethyl benzyl ammonium chloride 0.05 part
[0054] Monoethanolamine 0.2 part.
[0055] This is achieved through the following steps:
[0056] (1), the preparation of solution A: in 10m 3 Add water to the container, and slowly add carboxymethyl guar gum while stirring with a pump or a stirrer, and then add hydrocarbon emulsifier, trimethylhydroxypropyl quaternary ammonium salt clay stabilizer, dodecyl Continue to circulate or stir for 30 minutes after the addition of alkyl dimethyl benzyl ammonium chloride and monoethanolamine, so that the liquids can be fully mixed to form solution A.
[0057] (2) During fracturi...
Embodiment 2
[0059] First, the following materials are proportioned according to parts by weight:
[0060] 97.5 parts of water
[0061] Carboxymethyl guar gum 0.275 parts
[0062] Organic zirconium crosslinking agent 0.2 parts
[0063] Alkane sulfonate emulsifier 0.65 parts
[0064] Trimethylhydroxypropyl quaternary ammonium salt clay stabilizer 0.6 parts
[0065] Isothiazolinone 0.275 parts
[0066] 0.5 part of triethanolamine.
[0067] This is achieved through the following steps:
[0068] (1), the preparation of solution A: in 10m 3 Add water to the container, and slowly add carboxymethyl guar gum while stirring with a pump or a stirrer, and then add alkylsulfonate emulsifier and trimethylhydroxypropyl quaternary ammonium clay to stabilize Continue to circulate or stir for 30 minutes after adding the agent, isothiazolone and triethanolamine, so that the liquids can be fully mixed to form solution A.
[0069](2) During fracturing construction, while pumping solution A, mix solu...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com