Water-based polyurethane elastomer applied to sports ground
A water-based polyurethane and sports field technology, applied in the field of water-based polyurethane elastomers, can solve the problems of wasting oil resources, polluting the environment, wasting resources and the environment, and achieves the effects of green and environmental protection, good mechanical properties, and satisfactory drying time
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0018] A preparation method of a water-based polyurethane elastomer applied to a sports field, comprising the following steps:
[0019] 1) Add wetting and dispersing agent, anti-settling agent, defoaming agent, anti-mildew agent, leveling agent, matting agent and pH adjusting agent to 5-10 mass parts of water-based polyurethane resin, and disperse evenly;
[0020] 2) Add the remaining water-based polyurethane resin and stir evenly;
[0021] 3) Add color paste and stir well;
[0022] 4) Add filler and stir well;
[0023] 5) Add elastic rubber powder and stir well;
[0024] 6) Add thickener and stir well;
[0025] 7) Filter and package.
[0026] In the construction and application, for the one-component formula that does not contain the curing agent, it can be directly sprayed for construction. For the two-component formula containing the curing agent, in the construction and application, after the other raw materials are prepared according to the above steps, then follow th...
Embodiment 1
[0030] A kind of water-based polyurethane elastomer applied to sports field, its formula composition is as follows:
[0031] This formula is a one-component formula, and it can be directly scraped and applied after being configured according to the components.
Embodiment 2
[0033] A kind of water-based polyurethane elastomer applied to sports field, its formula composition is as follows:
[0034] This formula is a two-component formula, other components are prepared in advance, the curing agent is added before construction, and the construction can be done by scraping within 3 hours.
PUM
Property | Measurement | Unit |
---|---|---|
tensile strength | aaaaa | aaaaa |
Shore hardness | aaaaa | aaaaa |
water absorption | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com