Low-volatility high rosin flux and preparation method thereof
A rosin flux, low volatility technology, used in welding equipment, welding media, manufacturing tools, etc., can solve the problem of transformer feet, pole feet blackening, transformer feet, pole feet blackening, and increased flux concentration. problems, to achieve the effect of prolonging the service life, quickly and quickly tinning, and preventing air oxidation
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0050] A kind of low volatility high rosin soldering flux, by weight percentage, is made up of following components,
[0051] Rosin 60%
[0052] Carbon disulfide 37%
[0053] Tetrahydrofurfuryl Alcohol 1%
[0054] Triethylene glycol butyl ether 2%.
[0055] The preparation method of the present invention is:
[0056] The first step: adding carbon disulfide, tetrahydrofurfuryl alcohol and triethylene glycol butyl ether into a reactor with a stirring function by weight percentage;
[0057] Second step: add the rosin of corresponding weight percentage in reactor again;
[0058] The third step: fully stir until the rosin is completely dissolved, the mixture is brownish yellow, and the stirring density is 0.96±0.02 (g / cm 3 ) of the liquid.
[0059] The low-volatility high-rosin soldering flux of the present invention has a fast tinning speed and penetrates into the root of the soldering terminal to completely wrap the soldering terminal to avoid blackening of the soldering te...
Embodiment 2
[0061] A kind of low volatility high rosin soldering flux, by weight percentage, is made up of following components,
[0062] Rosin 50%
[0063] Carbon disulfide 42%
[0064] Tetrahydrofurfuryl Alcohol 3%
[0065] Triethylene glycol butyl ether 5%.
[0066] The preparation method of the low-volatility high-rosin flux of this embodiment is the same as that of Embodiment 1, and will not be repeated here.
Embodiment 3
[0068] A kind of low volatility high rosin soldering flux, by weight percentage, is made up of following components,
[0069] Rosin 68%
[0070] Carbon disulfide 31.85%
[0071] Tetrahydrofurfuryl alcohol 0.1%
[0072]Triethylene glycol butyl ether 0.05%.
[0073] The preparation method of the low-volatility high-rosin flux of this embodiment is the same as that of Embodiment 1, and will not be repeated here.