A preparation process and drug administration technology, which is applied in the field of preparation of anorectal drug ointment tubes, can solve problems such as the smoothness of the burr drug outlet, the neck of the tube is not soft enough, and complicated and numerous processes, and achieves process saving, good hand feeling, and easy to use. The effect of industrialization
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0025] combine figure 1 and figure 2 , Heat and knead polyethylene and 5% polyethylene mass masterbatch in the barrel of the extruder at a heating temperature of 120°C, extrude the obtained molten material into a straight tubular parison through a die, and set a Blow molding mold 4, when the straight tubular parison in the blow molding mold 4 reaches the required length, close the mold; feed compressed gas 5 for blow molding, the required pressure of compressed gas 5 is 0.6MPa, and the feeding time is 4s , to obtain the molded pipe body 6; when blow molding, inject cooling water with a temperature of -35°C into the cooling channel of the blow mold 4, and the flow rate of the cooling water is 10m 3 / h, cooling and shaping the formed pipe body 6; image 3 , the cooled forming tube body 6 is placed in the clamping mold 7, and the upper and lower ends of the forming tube body 6 are cut off, so as to respectively realize the water-cutting port of the drug delivery catheter 2 and...
Embodiment 2
[0027] Heat and knead the color masterbatch with 4% mass of polypropylene and polyethylene in the barrel of the extruder at a heating temperature of 170°C, and extrude the obtained molten material into a straight tubular parison through a die. Plastic mold, when the straight tubular parison in the blow mold reaches the required length, close the mold; feed compressed gas for blow molding, the pressure of the required compressed gas is 0.5MPa, and the time for feeding is 2s to obtain a molded pipe body ; When blow molding, inject cooling water with a temperature of -30°C into the cooling water channel of the blow molding mold, and the flow rate of the cooling water is 10m 3 / h, cooling and shaping the formed tube body; putting the cooled formed tube body into the clamping mold, cutting off the upper and lower ends of the formed tube body, so as to respectively realize the water cutting port of the drug delivery catheter 2 and the tube Cut the tail of the body tail; then put the...
Embodiment 3
[0029] Heat and knead polyvinyl chloride and 6% polyvinyl chloride color masterbatch in the barrel of the extruder at a heating temperature of 150°C, and extrude the obtained molten material into a straight tubular parison through the die head. There is a blow molding mold, when the straight tubular parison in the blow molding mold reaches the required length, the mold is closed; the compressed gas is fed into the blow molding, the required pressure of the compressed gas is 0.5MPa, and the feeding time is 3s, and the molding is obtained Pipe body; inject cooling water with a temperature of -28°C into the cooling water channel of the blow mold, and the flow rate of the cooling water is 11m 3 / h, cooling and shaping the formed tube body; putting the cooled formed tube body into the clamping mold, cutting off the upper and lower ends of the formed tube body, so as to respectively realize the water cutting port of the drug delivery catheter 2 and the tube Cut the tail at the tail ...
PUM