Composition comprising perlite and a polymer bearing a carbosiloxane dendrimer-based unit
A technology of carbosiloxane and vinyl polymers, which can be used in skin care preparations, cosmetics, dressing preparations, etc. It can solve the problems of difficult spreading and unpleasantness, and achieve the effect of improving the retention of matte effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0350] The liquid foundations of Example 1 and Example 2 can show that the dendritic silicone acrylates of the present invention provide better matte finish retention than silicone resins.
[0351]
[0352]
[0353] Process Example 1
[0354] Weigh the components of phase A1 in the main beaker, then stir the components by a Moritz stirrer (1000 rpm) while keeping at room temperature.
[0355] Next, phase A2 was added at room temperature with stirring using a Moritz stirrer (1000 rpm) until homogeneous.
[0356] Phase A3 was independently prepared by grinding the mixture of pigment and cyclohexasiloxane three times in a three-roll mill.
[0357] This phase A3 is then added with continuous stirring along with phases A4 and A5.
[0358] Prepare aqueous phase B separately by weighing butanediol and magnesium sulfate in a beaker, adding water preheated to 95°C.
[0359] Stir the aqueous phase using a magnetic bar until homogeneous.
[0360] Prepare the emulsion at room te...
Embodiment 2
[0364] Weigh the components of phase A1 in the main beaker, then stir the components by a Moritz stirrer (1000 rpm) while keeping at room temperature.
[0365] Phase A2 was previously prepared by dispersing the silicone resin in isododecane while stirring using a Rayneri stirrer (approximately 100 rpm) equipped with a deflocculating paddle.
[0366] Phase A2 was then added at room temperature with stirring using a Moritz stirrer (1000 rpm) until homogeneous.
[0367] Phase A3 was independently prepared by grinding the mixture of pigment and cyclohexasiloxane three times in a three-roll mill.
[0368] This phase A3 is then added with continuous stirring along with phases A4 and A5.
[0369] Aqueous phase B was also prepared separately by weighing butanediol and magnesium sulfate in a beaker, adding water preheated to 95°C.
[0370] Stir the aqueous phase using a magnetic bar until homogeneous.
[0371] Prepare the emulsion at room temperature: Inject the aqueous phase B into...
PUM
Property | Measurement | Unit |
---|---|---|
Size | aaaaa | aaaaa |
Size | aaaaa | aaaaa |
Size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology