An easy-to-clean, polyester-cotton blended technology, applied in textiles and papermaking, fiber processing, plant fibers, etc., can solve the problems of high price, difficult to clean thoroughly, easy to be contaminated with oil, etc., to achieve reasonable formula, improve easy removal dirty effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0012] Decontamination finishing agent for polyester-cotton blended fabrics, comprising the following raw materials in parts by mass: 15 parts of carboxymethyl cellulose, 5 parts of water-soluble silicone oil, 20 parts of water-based acrylate copolymer emulsion, 20 parts of glycerol, 80 parts of water share.
[0013] The preparation method of this example includes the following steps: according to the mass ratio, add carboxymethyl cellulose into water, stir evenly, then add water-soluble silicone oil and glycerol in turn, heat up to 50°C and stir for 20 minutes, add water-based acrylate Copolymerize the emulsion, continue to stir for 30 minutes, and wait for the solution to cool down to obtain the easy-to-decontaminate finishing agent for polyester-cotton blended fabrics
Embodiment 2
[0015] Decontamination finishing agent for polyester-cotton blended fabrics, comprising the following raw materials in parts by mass: 18 parts of carboxymethyl cellulose, 6 parts of water-soluble silicone oil, 25 parts of water-based acrylate copolymer emulsion, 25 parts of glycerol, and 90 parts of water share.
[0016] The preparation method of this example includes the following steps: according to the mass ratio, add carboxymethyl cellulose into water, stir evenly, then add water-soluble silicone oil and glycerol in turn, heat up to 55°C and stir for 20 minutes, add water-based acrylate Copolymerize the emulsion, continue to stir for 30 minutes, and wait for the solution to cool down to obtain the stain-removing finishing agent for polyester-cotton blended fabrics.
Embodiment 3
[0018] Decontamination finishing agent for polyester-cotton blended fabrics, comprising the following raw materials in parts by mass: 16 parts of carboxymethyl cellulose, 5.5 parts of water-soluble silicone oil, 22 parts of water-based acrylate copolymer emulsion, 23 parts of glycerol, 85 parts of water share.
[0019] The preparation method of this example includes the following steps: according to the mass ratio, add carboxymethyl cellulose into water, stir evenly, then add water-soluble silicone oil and glycerol in turn, heat up to 55°C and stir for 20 minutes, add water-based acrylate Copolymerize the emulsion, continue to stir for 30 minutes, and wait for the solution to cool down to obtain the stain-removing finishing agent for polyester-cotton blended fabrics.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com