[0008] (1) Take 4 kg of sodium petroleum sulfonate, 2 kg of polypropylene glycol diglycidyl ether, and 3 kg of dioctadecyl dimethyl ammonium chloride, heat the three components and mix and stir them, mix them evenly and set aside; (2) Take 230kg of water, add 3kg of alanine, 8kg of amyl alcohol, 2kg of potassium phosphate, and 2kg of sodium sulfate, and dissolve the alanine, amyl alcohol, potassium sulfate, and sodium sulfate in water evenly; (3) Add the mixed solution prepared in step (1) to the aqueous solution in step (2), stir with a mechanical stirring paddle at a stirring speed of 200rpm, and stir evenly; (4) Finally, put the finishing agent into a sealed tank and store .
Embodiment 2
[0010] (1) Take 6 kg of sodium petroleum sulfonate, 1 kg of polypropylene glycol diglycidyl ether, and 2 kg of dioctadecyl dimethyl ammonium chloride, heat the three ingredients, mix and stir, mix well and set aside; (2) Take 235kg of water, add 5kg of alanine, 7kg of amyl alcohol, 3kg of potassium phosphate, and 1kg of sodium sulfate, and dissolve the alanine, amyl alcohol, potassium sulfate, and sodium sulfate in water evenly; (3) Add the mixed solution prepared in step (1) to the aqueous solution in step (2), stir with a mechanical stirring paddle at a stirring speed of 250rpm, and stir evenly; (4) Finally, put the finishing agent into a sealed tank and store .
Embodiment 3
[0012] (1) Take 5kg of sodium petroleum sulfonate, 2kg of polypropylene glycol diglycidyl ether, and 2kg of dioctadecyldimethylammonium chloride, heat the three ingredients, mix and stir, mix well and set aside; (2) Take 240kg of water, add 4kg of alanine, 8kg of amyl alcohol, 2kg of potassium phosphate, and 1kg of sodium sulfate, and dissolve the alanine, amyl alcohol, potassium sulfate, and sodium sulfate in water evenly; (3) Add the mixed solution prepared in step (1) to the aqueous solution in step (2), stir with a mechanical stirring paddle at a stirring speed of 230rpm, and stir evenly; (4) Finally, put the finishing agent into a sealed tank and store .
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com