Color-changing composition in gel form
A color-changing composition and composition technology, applied in the field of color-changing compositions, can solve problems such as poor compatibility, difficult pigment wrapping transparency, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment approach
[0294] According to a preferred embodiment of the transparent gel of the present invention, comprising:
[0295] At least one polymer selected from the group consisting of acrylates / C10-30 alkyl acrylate crosspolymers such as Permulen TR-1, Permulen TR-2, Carbopol 1382, Carbopol ETD 2020, preferably in the form of A concentration of 0 to 10% by weight, more preferably 0 to 2% by weight; Carbomers, such as Synthalen K, Carbopol 980, preferably at a concentration of 0 to 10% by weight, more preferably 0 to 2% by weight; Ammonium acryloyldimethyltaurate / steareth-8 methacrylate copolymer, such as Aristoflex SNC, preferably in a concentration of 0 to 10% by weight, more preferably 0 to 2% by weight; acrylate Copolymers, such as Carbopol Aqua SF-1, preferably at a concentration of 0 to 10% by weight, more preferably 0 to 2% by weight; ammonium acryloyldimethyltaurate / steareth-25 formazan Acryloyl acrylate crosspolymer, such as Aristoflex HMS, preferably at a concentration of 0 to 1...
Embodiment
[0696] I Microcapsules
[0697] In the following, different examples of the preparation of microcapsules according to the invention are described in order to illustrate the invention.
example 1
[0698] Example 1 : Preparation of microcapsules with inner brown coating and outer white coating
[0699] Mannitol (spray-dried mannitol: Pearitol 100SD) was used as the core.
[0700] Add 120.0g of ceramide (ceramide PC 104) and 120.0g of hydrogenated lecithin (lipid S100-3) to a mixed solution of 1600.0g of dichloromethane and 1600.0g of ethanol, and dissolve completely at 40°C . 1260.0 g of iron oxide yellow, 252.0 g of iron oxide red, and 45.36 g of iron oxide black were added to the resulting mixture, and sufficiently dispersed using a homogenizer to prepare an internal color coating solution.
[0701] The mannitol of 347.70g is introduced into fluidized bed coating system (Glatt GPOG 1, bottom spray), as seed, is subjected to then coating internal color coating solution with the feed rate of 500ml / h, to obtain the coating with Granules of the mannitol core of the inner color layer.
[0702] Thereafter, 36.0 g of ceramide and 36.0 g of hydrogenated lecithin were adde...
PUM
| Property | Measurement | Unit |
|---|---|---|
| Size | aaaaa | aaaaa |
| Thickness | aaaaa | aaaaa |
| The average thickness | aaaaa | aaaaa |