High-strength ecological woodworking board and its manufacturing method
A manufacturing method and technology for woodworking boards, which are applied in the direction of manufacturing tools, wood-layered products, wood processing appliances, etc., can solve the problems of being easily eaten by moths, easily deformed, and insufficient in strength.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0087] A kind of manufacture method of high-strength ecological woodworking board, comprises the steps:
[0088] Step 1: Select a maple poplar middle board with a thickness of 0.35 cm, dry the above-mentioned maple poplar middle board at 70°C for 5 minutes, and let the above middle board dissipate heat to room temperature after drying;
[0089] Step 2: Sorting the middle plate that has been cooled to room temperature as described in step 1, using the middle plate with a hole diameter greater than 2 cm or a crack greater than 2 cm as the core blank, and using the middle plate with a hole diameter not greater than 2 cm. The middle plate with a centimeter or crack not greater than 2 cm is used as the upper middle plate 2 and the lower middle plate 3; the flatness of the middle plate used as the upper middle plate 2 and the lower middle plate 3 is greater than that of the middle plate used as the core blank flatness;
[0090] Step 3: Cutting the middle plate used as the core blan...
Embodiment 2
[0113] A kind of manufacture method of high-strength ecological woodworking board, comprises the steps:
[0114] Step 1: Select a maple poplar middle board with a thickness of 0.37 cm, dry the above-mentioned maple poplar middle board at 90°C for 5 minutes, and let the above middle board cool down to room temperature after drying;
[0115] Step 2: Sorting the middle plate that has been cooled to room temperature as described in step 1, using the middle plate with a hole diameter greater than 2 cm or a crack greater than 2 cm as the core blank, and using the middle plate with a hole diameter not greater than 2 cm. The middle plate with a centimeter or crack not greater than 2 cm is used as the upper middle plate 2 and the lower middle plate 3; the flatness of the middle plate used as the upper middle plate 2 and the lower middle plate 3 is greater than that of the middle plate used as the core blank flatness;
[0116] Step 3: Cutting the middle plate used as the core blank aft...
Embodiment 3
[0139] A kind of manufacture method of high-strength ecological woodworking board, comprises the steps:
[0140]Step 1: Select a maple poplar middle board with a thickness of 0.36 cm, dry the above-mentioned maple poplar middle board at 80°C for 5 minutes, and let the above middle board cool down to room temperature after drying;
[0141] Step 2: Sorting the middle plate that has been cooled to room temperature as described in step 1, using the middle plate with a hole diameter greater than 2 cm or a crack greater than 2 cm as the core blank, and using the middle plate with a hole diameter not greater than 2 cm. The middle plate with a centimeter or crack not greater than 2 cm is used as the upper middle plate 2 and the lower middle plate 3; the flatness of the middle plate used as the upper middle plate 2 and the lower middle plate 3 is greater than that of the middle plate used as the core blank flatness;
[0142] Step 3: Cut the middle plate used as the core blank after th...
PUM
| Property | Measurement | Unit |
|---|---|---|
| thickness | aaaaa | aaaaa |
| width | aaaaa | aaaaa |
| width | aaaaa | aaaaa |
Abstract