A technology for writing newsprint in water and a manufacturing process, which is applied to reusable writing boards, paper, papermaking, etc., can solve the problems of rough surface, high cost, cumbersome manufacturing procedures, etc., and achieves low price, good imitation effect, Good writing feel
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0041] A kind of manufacturing process of special water writing newsprint for painting and calligraphy practice, comprises the following steps:
[0042] Step 1: using raw pulp or waste paper as raw material, through pulping, pulping, and papermaking, to obtain diluted pulp;
[0043] Step 2: adding carbon black to the slurry described in step 1 to make a black slurry;
[0044] Step 3: make the black pulp described in step 2 pass through the headbox to distribute the pulp, and the wire part is formed; the concentration of the online pulp is 0.9wt%-1.5wt%, and the pH value of the online pulp is 6-7.5;
[0045] Step 4: Make the pulp formed in the wire part described in step 3 through rolling and compound pressing, dry it before drying, carry out flat decoration on the surface, dry it after drying, and roll the paper to become black newsprint; soft calendering pressure 15- 65kN / m, the temperature of the soft calender is 60-95°C; the paper grammage of the black newsprint is 45-350g / m...
Embodiment 2
[0049] A kind of manufacturing process of special water writing newsprint for painting and calligraphy practice, comprises the following steps:
[0050] Step 1: using raw pulp or waste paper as raw material, through pulping, pulping, and papermaking, to obtain diluted pulp;
[0051] Step 2: adding carbon black to the slurry described in step 1 to make a black slurry;
[0052] Step 3: make the black pulp described in step 2 pass through the headbox to distribute the pulp, and the wire part is formed; the concentration of the online pulp is 0.9wt%-1.5wt%, and the pH value of the online pulp is 6-7.5;
[0053] Step 4: Make the pulp formed in the wire part described in step 3 through rolling and compound pressing, dry it before drying, carry out flat decoration on the surface, dry it after drying, and roll the paper to become black newsprint; soft calendering pressure 15- 65kN / m, the temperature of the soft calender is 60-95°C; the paper grammage of the black newsprint is 45-350g...
Embodiment 3
[0058] A kind of manufacturing process of special water writing newsprint for painting and calligraphy practice, comprises the following steps:
[0059] Step 1: using raw pulp or waste paper as raw material, through pulping, pulping, and papermaking, to obtain diluted pulp;
[0060] Step 2: adding carbon black to the slurry described in step 1 to make a black slurry;
[0061] Step 3: make the black pulp described in step 2 pass through the headbox to distribute the pulp, and the wire part is formed; the concentration of the online pulp is 0.9wt%-1.5wt%, and the pH value of the online pulp is 6-7.5;
[0062] Step 4: Make the pulp formed in the wire part described in step 3 through rolling and compound pressing, dry it before drying, carry out flat decoration on the surface, dry it after drying, and roll the paper to become black newsprint; soft calendering pressure 15- 65kN / m, the temperature of the soft calender is 60-95°C; the paper grammage of the black newsprint is 45-350g...