A method of preparing micro-lattice pattern on PMMA light guide plate
A micro-lattice and light guide plate technology, applied in the field of light guide plates, can solve the problems of low production efficiency, high cost, uneven astigmatism, etc., and achieve the effects of high production efficiency, reduced volatilization, and small size
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0039] S11. Design the circular micro-dot matrix in the computer, and print the circular micro-dot matrix on the polyvinyl alcohol film with a high-precision inkjet printer;
[0040] S12. adopt the method for roller coating to coat polyurethane coating on PMMA light guide plate substrate;
[0041] S13. Paste the polyvinyl alcohol film on the PMMA light guide plate coated with polyurethane coating, the surface containing the micro-lattice pattern is in contact with the coating, and dry it in a drying oven at 50° C. for 5 minutes;
[0042] S14. Soak the PMMA light guide plate affixed with the polyethylene film in water for 2 minutes to remove the polyvinyl alcohol film, and obtain the circular micro-dot matrix required by the design on the PMMA light guide plate.
Embodiment 2
[0044] S21. Design the diamond-shaped micro-dot matrix in the computer, and use a high-precision inkjet printer to print the diamond-shaped micro-dot matrix on the polyvinyl alcohol film;
[0045] S22. adopt dipping method to coat epoxy resin coating on PMMA light guide plate base material;
[0046] S23. Paste the polyvinyl alcohol film on the PMMA light guide plate coated with epoxy resin coating, the surface containing the micro-lattice pattern is in contact with the coating, and dry in a drying oven at 70°C for 3 minutes;
[0047] S24. Soak the PMMA light guide plate affixed with polyethylene film in water for 1 minute to remove the polyvinyl alcohol film, and obtain the diamond-shaped micro-lattice matrix required by the design on the PMMA light guide plate.
Embodiment 3
[0049] S31. Design a rectangular micro-dot matrix in the computer, and print the rectangular micro-dot matrix on the polyvinyl alcohol film with a high-precision inkjet printer;
[0050] S32. Coating a phenolic resin coating on the PMMA light guide plate substrate by spraying;
[0051] S33. Paste the polyvinyl alcohol film on the PMMA light guide plate coated with phenolic resin coating, the surface containing the micro-lattice pattern is in contact with the coating, and after drying for 4 minutes in a drying oven at a temperature of 60 ° C;
[0052] S34. Soak the PMMA light guide plate with the polyethylene film in water for 2 minutes to remove the polyvinyl alcohol film, and obtain the rectangular micro-dot matrix required by the design on the PMMA light guide plate.