[0022] Fine art paints consist of the following components:
[0023] 8 parts of ocher, 15 parts of calcium carbonate, 1 part of sodium benzoate, 7 parts of mercury sulfide, 7 parts of cadmium sulfate, 20 parts of polyurethane modified epoxy resin emulsion, 15 parts of pigment powder, 20 parts of distilled water, 18 parts of thickener and color Microparticles 21 parts.
[0024] The preparation method of art paint, comprises the following steps:
[0025] A, the polyurethane modified epoxy resin emulsion was stirred for 30 minutes for subsequent use;
[0026] B. Mix ocher, calcium carbonate, sodium benzoate, mercury sulfide, cadmium sulfate, pigment powder and distilled water and stir for 20 minutes for later use;
[0027] C, mixing the base material in step A with the mixture in step B and grinding to form a pigment body;
[0028] D. At the same time, add the thickener to the pigment body and stir for 10 minutes;
[0029] E. Finally, add color micro-particles and stir to for...
Embodiment 2
[0031] Fine art paints consist of the following components:
[0032] 9 parts of ocher, 5 parts of calcium carbonate, 1.5 parts of sodium benzoate, 15 parts of mercury sulfide, 6 parts of cadmium sulfate, 27 parts of polyurethane modified epoxy resin emulsion, 19 parts of pigment powder, 35 parts of distilled water, 18 parts of thickener and color Microparticles 26 parts.
[0033] The preparation method of art paint, comprises the following steps:
[0034] A, the polyurethane modified epoxy resin emulsion was stirred for 30 minutes for subsequent use;
[0035] B. Mix ocher, calcium carbonate, sodium benzoate, mercury sulfide, cadmium sulfate, pigment powder and distilled water and stir for 20 minutes for later use;
[0036] C, mixing the base material in step A with the mixture in step B and grinding to form a pigment body;
[0037] D. At the same time, add the thickener to the pigment body and stir for 10 minutes;
[0038] E. Finally, add color micro-particles and stir to ...
Embodiment 3
[0040] Fine art paints consist of the following components:
[0041] 7 parts of ocher, 10 parts of calcium carbonate, 1 part of sodium benzoate, 7 parts of mercury sulfide, 4 parts of cadmium sulfate, 22 parts of polyurethane modified epoxy resin emulsion, 28 parts of pigment powder, 27 parts of distilled water, 15 parts of thickener and color Microparticles 22 parts.
[0042] The preparation method of art paint, comprises the following steps:
[0043] A, the polyurethane modified epoxy resin emulsion was stirred for 30 minutes for subsequent use;
[0044] B. Mix ocher, calcium carbonate, sodium benzoate, mercury sulfide, cadmium sulfate, pigment powder and distilled water and stir for 20 minutes for later use;
[0045] C, mixing the base material in step A with the mixture in step B and grinding to form a pigment body;
[0046] D. At the same time, add the thickener to the pigment body and stir for 10 minutes;
[0047] E. Finally, add color micro-particles and stir to for...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com