Manufacturing method of leather capable of preventing and treating athlete's foot
A production method and leather technology, applied in leather manufacturing, medical preparations containing active ingredients, leather drying, etc., can solve the problems of ineffective treatment, troublesome treatment methods, side effects, etc., and achieve long-lasting performance, simple process, Strong sweat-wicking effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0056] Step a. The medicine is distributed according to the following weight ratios:
[0057]Nepeta panicle 10.8%, Fangfeng 9.7%, Alum 18.8%, Saponaria 16.1%, Dafengzi 13.4%, Digupi 9.7%, Wujiapi 13.4%, Safflower 8.1%
[0058] Afterwards, the medicine is ground into a powder for subsequent use.
[0059] Step b. After the salt-wet cowhide is depilated and gelatinized, enter the tanning stage, immerse the salt-wet cowhide in water, then add the tanning liquid and the medicinal powder in step a into water to form a mixed solution, and intermittently stir the mixed solution, Stir every 1h, stop for 20min, and continue stirring intermittently for 8h, wherein every 2500g of water is added with 186g of medicinal powder. The stirring speed is 4 revolutions per minute, and the temperature of the mixed solution is kept between 30°C and 45°C. Tanning solutions for tanning include protein solutions and oils.
[0060] Step c. After stirring, let it stand for 6 hours. The temperature of ...
Embodiment 2
[0064] Step a. The medicine is distributed according to the following weight ratios:
[0065] Nepeta panicle 9%, Fangfeng 8%, Alum 20%, Saponin 18%, Dafengzi 12%, Digupi 8%, Wujiapi 17%, Safflower 8%.
[0066] Afterwards, the medicine is ground into a powder for subsequent use.
[0067] Step b. After the salt-wet cowhide is depilated and gelatinized, enter the tanning stage, immerse the salt-wet cowhide in water, then add the tanning liquid and the medicinal powder in step a into water to form a mixed solution, and intermittently stir the mixed solution, Every stirring for 1 hour, stop for 15 minutes, and continue intermittent stirring for 12 hours, wherein every 2500 grams of water is added with 160 grams of medicinal powder. The stirring speed is 6 revolutions per minute, and the temperature of the mixed solution is kept between 30°C and 45°C. Tanning solutions for tanning include protein solutions and oils.
[0068] Step c. After stirring, let it stand for 4 hours. The t...
Embodiment 3
[0072] Step a. The medicine is distributed according to the following weight ratios:
[0073] Nepeta 12%, Fangfeng 11%, Alum 17%, Saponin 14%, Dafengzi 13%, Digupi 9%, Wujiapi 18%, Safflower 6%.
[0074] Afterwards, the medicine is ground into a powder for subsequent use.
[0075] Step b. After the salt-wet cowhide is depilated and gelatinized, enter the tanning stage, immerse the salt-wet cowhide in water, then add the tanning liquid and the medicinal powder in step a into water to form a mixed solution, and intermittently stir the mixed solution, Every stirring for 1h, stop for 25min, and continue to stir intermittently for 12h, wherein every 2500g of water is added with 210g of medicinal powder. The stirring speed is 5 revolutions per minute, and the temperature of the mixed solution is kept between 30°C and 45°C. Tanning solutions for tanning include protein solutions and oils.
[0076] Step c. After stirring, let it stand for 5 hours. The temperature of the mixed solut...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com