A kind of lens paper and preparation method thereof
A technology of lens paper and raw paper, which is applied in paper, papermaking, paper machines, etc., can solve the problems of lens paper not soft and easy to scratch the lens, and achieve the effect of improving water absorption capacity and anti-oxidation capacity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0009] Embodiment 1: A kind of lens paper, it comprises by weight: 10 parts of green sandalwood, 5 parts of rice straw, 0.2 part of aloe extract, 1.2 parts of cellulose acetate, 4 parts of starch and 6 parts of deionized water.
[0010] A method for preparing lens paper, which includes the following steps: (1), mixing 10 parts of green sandalwood and 5 parts of straw, soaking in 6 parts of deionized water for 30 minutes, and the soaking temperature is 40 °C; The mixture of sandalwood and rice straw is sent to the beater for 20 minutes to form the original slurry, during which 1.2 parts of cellulose acetate are added; (3), 0.2 parts of the aloe extract is heated to 50 °C, then added to the original slurry, stirred evenly, distilled and concentrated to the original volume 1 / 3 to obtain the pulp; (4), the pulp is scooped, dried and cut to form raw paper, and 4 parts of starch are evenly coated on the raw paper, and then smoked with steam for 1 hour to obtain lens paper.
Embodiment 2
[0011] Embodiment 2: A kind of lens paper, it comprises by weight: 15 parts of green sandalwood, 7 parts of rice straw, 0.4 part of aloe extract, 1.4 parts of cellulose acetate, 6 parts of starch and 8 parts of deionized water.
[0012] A preparation method of lens paper, which comprises the following steps: (1), mixing 15 parts of green sandalwood and 7 parts of rice straw, soaking in 8 parts of deionized water for 35 minutes, and the soaking temperature is 45 °C; The mixture of sandalwood and rice straw is sent to the beater for 25 minutes to form the original slurry, during which 1.4 parts of cellulose acetate are added; (3), 0.4 parts of the aloe extract is heated to 55 °C, then added to the original slurry, stirred evenly, distilled and concentrated to the original volume 1 / 3 to get the pulp; (4) After scooping, drying and cutting the pulp to form raw paper, 4-8 parts of starch are evenly coated on the raw paper and then smoked with steam for 2 hours to obtain lens paper. ...
Embodiment 3
[0013] Embodiment 3: A kind of lens paper, it comprises by weight: 20 parts of green sandalwood, 10 parts of rice straw, 0.6 part of aloe extract, 1.6 parts of cellulose acetate, 8 parts of starch and 10 parts of deionized water.
[0014] A method for preparing lens paper, which includes the following steps: (1), mixing 20 parts of green sandalwood and 10 parts of straw, soaking in 10 parts of deionized water for 40 minutes, and the soaking temperature is 50 °C; The mixture of sandalwood and rice straw is sent to the beater for 30 minutes to form the original slurry, during which 1.6 parts of cellulose acetate are added; (3), 0.6 parts of the aloe extract is heated to 60 °C, then added to the original slurry, stirred evenly, distilled and concentrated to the original volume 1 / 3 to obtain the pulp; (4), the pulp is scooped, dried and cut to form raw paper, 8 parts of starch are evenly coated on the raw paper, and then smoked with steam for 3 hours to obtain lens paper.