Seal welding technology for electroplating anode bag
A sealing welding, anode bag technology, applied in welding equipment, non-electric welding equipment, manufacturing tools, etc., can solve the problems of copper slag leakage, affecting quality, polluting electroplating tanks, etc., to achieve the effect of ensuring the amount of electrolyte
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] A sealing and welding process for an anode bag for electroplating, comprising the following steps: (1) selecting a corresponding ultrasonic welding mold according to the size and shape of the anode bag; (2) fixing the anode bag to be welded into the welding mold; (3) pressing Welding: In the process of ultrasonic pressing, the ultrasonic welding time is 60S-300S, and the hardening time after welding is 0.3S-10S; the pressing width is 3mm-10mm.
[0017] The edge of the anode bag is sealed by the process of ultrasonic welding and pressing to ensure its tightness without any leakage, effectively ensure the amount of electrolyte, and prevent the pollution of the electrolytic cell. Through repeated tests, the sealing performance is the best when the time for welding the edge of the anode bag is 60S-300S, and the hardening time after welding is 0.3S-10S. According to different sizes of anode bags, the width of the lamination will change accordingly, generally between 3mm-10mm...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap