Deoiling phosphating solution and preparation method thereof
A technology of phosphating solution and zinc dihydrogen phosphate, which is applied in the coating process of metal materials, can solve the problems of few breakthroughs in phosphating technology, incomplete clarification, and high energy consumption, and achieve a dense and uniform phosphating film , low cost and simple preparation method
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0011] The degreasing and phosphating solution of this embodiment is prepared from the following components by weight: 3-6 parts of hydroxylamine sulfate, 2 parts of sodium alkylarylsulfonate, 1 part of hexamethylenetetramine, zinc dihydrogen phosphate 12 parts, 12 parts of N-(phosphonomethyl) glycine isopropylamine salt, 6 parts of sodium lauryl sulfate, 2 parts of sodium carboxymethyl starch, 10 parts of linolenic acid, 3 parts of dinitropentamethylenetetramine parts, 40 parts of water, 15 parts of sodium fluoroborate.
[0012] Weigh each component according to the above weight ratio, then mix and stir, and stir evenly to completely dissolve each component, so as to obtain the oil-removing phosphating solution.
[0013] In the present invention, the surface of the metal workpiece can be treated by directly soaking and spraying, and then naturally dried to obtain a phosphating film.
Embodiment 2
[0015] The degreasing and phosphating solution of the present embodiment is prepared from the following components in parts by weight: 3-6 parts of hydroxylamine sulfate, 5 parts of sodium alkylarylsulfonate, 6 parts of hexamethylenetetramine, zinc dihydrogen phosphate 16 parts, N-(phosphonomethyl)glycine isopropylamine salt 15 parts, sodium lauryl sulfate 9 parts, carboxymethyl starch 4 parts, linolenic acid 14 parts, dinitropentamethylenetetramine 6 parts , 60 parts of water, 17 parts of sodium fluoroborate, and 8 parts of sodium fatty acid.
[0016] Weigh each component according to the above weight ratio, then mix and stir, and stir evenly to completely dissolve each component, so as to obtain the oil-removing phosphating solution.
[0017] In the present invention, the surface of the metal workpiece can be treated by directly soaking and spraying, and then naturally dried to obtain a phosphating film.
Embodiment 3
[0019] The degreasing and phosphating solution of this embodiment is prepared from the following components by weight: 3-6 parts of hydroxylamine sulfate, 2 parts of sodium alkylarylsulfonate, 1 part of hexamethylenetetramine, zinc dihydrogen phosphate 12 parts, 12 parts of N-(phosphonomethyl) glycine isopropylamine salt, 6 parts of sodium lauryl sulfate, 2 parts of sodium carboxymethyl starch, 10 parts of linolenic acid, 3 parts of dinitropentamethylenetetramine 40 parts of water, 15 parts of sodium fluoroborate, 5 parts of sodium fatty acid, 3 parts of ethylenediaminetetraacetic acid.
[0020] Weigh each component according to the above weight ratio, then mix and stir, and stir evenly to completely dissolve each component, so as to obtain the oil-removing phosphating solution.
[0021] In the present invention, the surface of the metal workpiece can be treated by directly soaking and spraying, and then naturally dried to obtain a phosphating film.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com