A bearing cage and light decoration technology, which is applied in shaft cleaning, bearing cleaning, bearing and other directions, can solve the problem that the silver plating quality of the bearing cage cannot meet the technical requirements of the product, increase the cost of bearing production, etc., and achieve saving of silver liquid funds, Improved production efficiency and improved bearing performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
specific Embodiment approach 1
[0018] Specific implementation mode 1: The bearing cage finishing cleaning method of this embodiment, the steps of the bearing cage finishing cleaning method are as follows:
[0019] Step 1. Using oblique triangular brown corundum with a particle size of 90-100 as the light decoration material;
[0020] Step 2. According to the pocket size of the bearing cage, select the corresponding specification of the finishing material:
[0021] When the pocket size of the bearing cage is 5-10mm, the specification of the selected glossy material is 12X15mm;
[0022] When the size of the pocket of the bearing cage is 10-18mm, the specification of the selected glossy material is 20X23mm;
[0023] When the size of the pocket of the bearing cage is 18-30mm, the specification of the selected glossy material is 33X35mm;
[0024] Step 3. Use the existing finishing machine, the weight of the finishing material is 175kg, and the amount of finishing fluid is 800-1000ml of anti-rust solution;
[...
specific Embodiment approach 2
[0027] Specific implementation mode 2: After the finishing in step 4 of this implementation mode, place the bearing cage in the anti-rust tank, remove it after 1 minute, and tilt the bearing cage to stand for 0.5-1 minute. In this way, the surface quality of the bearing cage after silver plating is improved. Other steps are the same as in the first embodiment.
specific Embodiment approach 3
[0028] Embodiment 3: The finishing liquid in step 3 of this embodiment is a mixture of sodium nitrite and water, and the weight ratio of sodium nitrite to water is 1:2. In this way, the anti-rust effect is good. Other steps are the same as those in Embodiment 1 or 2.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com