Embodiment 2
[0034] The heat dissipation coating of the present invention comprises the following components by weight:
[0035]
[0036] The heat dissipation coating of the present invention is prepared by the following method, comprising the steps of:
[0037] A, water-based acrylic resin, polycarbonate-type water-based polyurethane, silicone resin containing modified nanoparticles, silica sol and water are mixed and stirred evenly;
[0038] B. Add thermally conductive fillers and additives in the state of stirring, and stir evenly to obtain a dispersion system;
[0039] C. Put the dispersion system in step B into a paint grinder and grind it to 30-50 μm, and disperse evenly by ultrasonic.
[0040] Wherein said polycarbonate type waterborne polyurethane is prepared by the following method:
[0041] Add 1000 parts by weight of polycarbonate diol into a container with a stirrer, raise the temperature to 90°C, distill under reduced pressure for 0.5 hours, cool down to 70°C, add 280 par...
Embodiment 3
[0049] The heat dissipation coating of the present invention comprises the following components by weight:
[0050]
[0051] The heat dissipation coating of the present invention is prepared by the following method, comprising the steps of:
[0052] A, water-based acrylic resin, polycarbonate-type water-based polyurethane, silicone resin containing modified nanoparticles, silica sol and water are mixed and stirred evenly;
[0053] B. Add thermally conductive fillers and additives in the state of stirring, and stir evenly to obtain a dispersion system;
[0054] C. Put the dispersion system in step B into a paint grinder and grind it to 30-50 μm, and disperse evenly by ultrasonic.
[0055] Wherein said polycarbonate type waterborne polyurethane is prepared by the following method:
[0056] Add 1000 parts by weight of polycarbonate diol into a container with a stirrer, raise the temperature to 90°C, distill under reduced pressure for 0.5 hours, cool down to 70°C, add 280 par...
Embodiment 4
[0064] The heat dissipation coating of the present invention comprises the following components by weight:
[0065]
[0066] The heat dissipation coating of the present invention is prepared by the following method, comprising the steps of:
[0067] A, water-based acrylic resin, polycarbonate-type water-based polyurethane, silicone resin containing modified nanoparticles, silica sol and water are mixed and stirred evenly;
[0068] B. Add thermally conductive fillers and additives in the state of stirring, and stir evenly to obtain a dispersion system;
[0069] C. Put the dispersion system in step B into a paint grinder and grind it to 30-50 μm, and disperse evenly by ultrasonic.
[0070] Wherein said polycarbonate type waterborne polyurethane is prepared by the following method:
[0071] Add 1000 parts by weight of polycarbonate diol into a container with a stirrer, raise the temperature to 90°C, distill under reduced pressure for 0.5 hours, cool down to 70°C, add 280 par...
PUM