The method of making microfilament fibrous into silk-like cotton through air-lay
An air-laid and filament fiber technology, applied in the field of imitation silk cotton, can solve the problems of environmental pollution, non-recyclable utilization, waste of resources, etc., and achieve the effects of reducing environmental pollution, saving costs, and effectively distributing
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0020] The method for preparing superfine filament fiber air-laid silk-like cotton is characterized in that it comprises the following steps:
[0021] a) Preparation of viscose fiber
[0022] Take the conjugate filament fiber and add it to the spinning dope, stir it evenly with a mixer, and then wet spin it to make viscose fiber; the conjugate filament fiber is a conjugate of water-soluble thermoplastic resin and water-insoluble thermoplastic resin Filament fiber
[0023] b) Ingredients
[0024] The viscose fiber prepared in step 1) is mixed with the low-melting fiber extracted from waste cotton and then mixed by a multi-layer flat method. The ratio of the two according to the mass ratio is: multifunctional viscose fiber: 90 parts , 10 parts of low melting point fiber;
[0025] c) Remove water-soluble thermoplastic resin
[0026] Put the ingredients obtained in step 2) into a hydrophilic solvent, the soaking temperature is 20°C, the soaking time is 2 hours, the temperature rises by 10°...
Embodiment 2
[0032] The preparation method of superfine filament fiber air-laid silk-like cotton includes the following steps:
[0033] a) Preparation of viscose fiber
[0034] Take the conjugate filament fiber and add it to the spinning dope, stir it evenly with a mixer, and then wet spin it to make viscose fiber; the conjugate filament fiber is a conjugate of water-soluble thermoplastic resin and water-insoluble thermoplastic resin Filament fiber
[0035] b) Ingredients
[0036] The viscose fiber prepared in step 1) is mixed with the low-melting fiber extracted from waste cotton and then mixed by a multi-layer flat method. The ratio of the two according to the mass ratio is: multifunctional viscose fiber: 80 parts, 20 parts of low melting point fiber;
[0037] c) Remove water-soluble thermoplastic resin
[0038] Put the ingredients obtained in step 2) into a hydrophilic solvent, the soaking temperature is 30°C, the soaking time is 1 hour, and the temperature is increased by 30°C every half an hou...
PUM
| Property | Measurement | Unit |
|---|---|---|
| Fiber length | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information