[0012] In a 500mL four-neck flask equipped with a stirrer, heating device, thermometer, dropping funnel and dehydration device, add 250g (containing 0.8mol carboxyl group) polymeric acid, start stirring and feed nitrogen, then start heating, and heat to At 160°C, put 86.4g (containing 0.4mol amine) of D400 (the structural formula is NH 2 CH (CH 3 ) CH 2 (OR) m CH 2 NH 2 , where R is isopropyl, m is 6.1) put it into the dropping funnel, add D400 dropwise into the four-necked flask under stirring and at a temperature of 160°C, and continue to heat up to 180°C for reaction after the dropwise addition is completed , keep this temperature until no more water is produced, continue to react for 30 minutes, and then cool down to 50°C after the reaction, to obtain a viscosity-increasing and shear-increasing agent for oil-based drilling fluid.
Embodiment 2
[0014] In a 500mL four-neck flask equipped with a stirrer, heating device, thermometer, dropping funnel and dehydration device, add 250g (containing 0.8mol carboxyl group) polymeric acid, start stirring and feed nitrogen, then start heating, and heat to At 160°C, put 51.84g (containing 0.24mol amine) of D400 (the structural formula is NH 2 CH (CH 3 ) CH 2 (OR) m CH 2 NH 2 , where R is isopropyl, m is 6.1) put it into the dropping funnel, add D400 dropwise into the four-necked flask under stirring and at a temperature of 160°C, and continue to heat up to 180°C for reaction after the dropwise addition is completed , keep this temperature until no more water is generated, continue to react for 30 minutes, and then cool down to 50°C after the reaction, to obtain a viscosity-increasing and shear-increasing agent for oil-based drilling fluid.
Embodiment 3
[0016] Add 125g (containing 0.4mol carboxyl group) polymeric acid into the four-necked flask described in Example 1, start stirring and feed nitrogen, then start heating, when heated to 160°C, put 200g (containing 0.2mol amine group) D2000 (structural formula is NH 2 CH (CH 3 ) CH 2 (OR) m CH 2 NH 2 , where R is isopropyl, m is 33) put it into the dropping funnel, add D2000 dropwise into the four-necked flask under stirring and at a temperature of 160°C, and continue to heat up to 200°C for reaction after the dropwise addition is completed , keep this temperature until no more water is produced, continue to react for 30 minutes, and then cool down to 50°C after the reaction, to obtain a viscosity-increasing and shear-increasing agent for oil-based drilling fluid.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com