Easy-defoaming photosensitive plastic paint and manufacturing method thereof
A resin and propylene glycol technology, used in polyester coatings, coatings, etc., can solve problems such as poor defoaming of photosensitive plastic paint, and achieve the effect of preventing construction and ensuring rapidity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment Construction
[0010] 30 kg of dehydrated malic acid resin, 10 kg of propylene glycol, 0.01 kg of polyethylene glycol (600), 1 kg of ultrafine silicon dioxide, 2 kg of polyamide wax (n-butanol, naphtha mixture), 1250 mesh of talcum powder 2 kg, 15 kg of o-phthalic unsaturated polyester resin, 0.1 kg of polyvinyl butyral, 10 kg of styrene, and 2 kg of photosensitive plastic initiator (D1173). Acid resin polymer (solid content 80%), propylene glycol, polyethylene glycol (600), ultrafine silicon dioxide, polyamide wax (n-butanol, petroleum naphtha mixture), talcum powder 1250 mesh, and continue to stir for 90 minutes , then add o-phthalic unsaturated polyester resin, polyvinyl butyral, styrene, defoaming polysiloxane and polyethylene glycol hydrophobic solid mixture, continue to stir for 30 minutes, and finally add photosensitive plastic initiator ( D1173), keep away from light.
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More