[0035] A waterproof, oil-proof, breathable clothing, prepared by the method of the following steps:
[0036] (1) Fluffy treatment: add soap oil and soda ash to 70°C water to form a mixed solution; then put the garment into the mixed solution and rinse for 15 minutes; then rinse with clean water, dehydrate and then dry;
[0037] (2) Lamination treatment: mix fluorine compound, penetrant and water, soak the fluffy treated garment obtained in step (1) in the mixed solution of fluorine compound, penetrant and water for 20 minutes, then dehydrate, and then Dried to 20% of the clothing with liquid;
[0038] (3) Film-forming treatment: put the garment after lamination treatment obtained in step (2) in a high-temperature furnace at 170° C. for 3 minutes and take it out;
[0039] (4) softening treatment: put soft oil into water and mix evenly to form soft oil water for subsequent use; put the film-forming garment obtained in step (3) into the soft oil water for rinsing, dehydration, and...
Embodiment 2
[0041] A waterproof, oil-proof, breathable clothing, prepared by the method of the following steps:
[0042] (1) fluffy treatment: first water is heated to 75 ℃, with 200g water, described 5g soap oil is dissolved as soap oil aqueous solution, then with 200g water, 10g described soda ash is dissolved into soda ash aqueous solution, finally described soap oil aqueous solution Add the soda ash aqueous solution to the remaining 4.6kg of water to form a mixed solution; then put the clothes into the mixed solution and rinse for 15 minutes; then rinse with clear water, dry after dehydration;
[0043] (2) Lamination treatment: Mix 350g of fluorine compound, 5g of penetrant and 5kg of water at 40°C, soak the fluffy treated garment obtained in step (1) in the mixture of fluorine compound, penetrant and water 10-30 minutes, then dehydrate to 65% of the liquid on the garment, and then dry to 20% of the liquid on the garment;
[0044] (3) Film-forming treatment: put the garment after lam...
Embodiment 3
[0047] A waterproof, oil-proof, breathable clothing, prepared by the method of the following steps:
[0048] (1) fluffy treatment: first water is heated to 65 ℃, with 200g water, described 5g soap oil is dissolved as soap oil aqueous solution, then with 200g water, 10g described soda ash is dissolved into soda ash aqueous solution, finally described soap oil aqueous solution Add the soda ash aqueous solution to the remaining 4.6kg of water to form a mixed solution; then put the clothes into the mixed solution and rinse for 15 minutes; rinse twice with water, each time for 10 minutes, and dry after dehydration;
[0049] (2) Lamination treatment: Mix 350g of fluorine compound, 5g of penetrant and 5kg of water at 40°C, soak the fluffy treated garment obtained in step (1) in the mixture of fluorine compound, penetrant and water 10-30 minutes, then dehydrate to 65% of the liquid on the garment, and then dry to 20% of the liquid on the garment;
[0050] (3) Film-forming treatment: ...
PUM

Abstract
Description
Claims
Application Information

- R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com