Waterproof putty powder and preparation method thereof
A technology of putty powder and rubber powder, applied in the field of putty powder, can solve problems such as poor waterproof effect of putty powder, achieve high waterproof effect, improve work efficiency, and reduce drying time
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0023] A kind of waterproof putty powder, in parts by weight, comprises the following components:
[0024] 40 parts of white cement, 35 parts of talcum powder, 30 parts of ash calcium, 1 part of cellulose ether, 2 parts of water-resistant rubber powder, 10 parts of bentonite, 1 part of cellulose, 1 part of thickener, and 0.1 part of defoamer.
[0025] Its preparation method comprises the following steps:
[0026] 1) Add water to white cement, talcum powder, lime calcium, cellulose ether, water-resistant rubber powder, bentonite, cellulose, thickener, and defoamer, and stir well to mix evenly.
[0027] 2) After the mixed material is dried by a putty powder dryer, it can be packaged for use.
Embodiment 2
[0029] A kind of waterproof putty powder, in parts by weight, comprises the following components:
[0030] 55 parts of white cement, 50 parts of talcum powder, 40 parts of lime calcium, 3 parts of cellulose ether, 5 parts of water-resistant glue powder, 15 parts of bentonite, 3 parts of cellulose, 2 parts of thickener, and 0.4 part of defoamer.
[0031] Its preparation method comprises the following steps:
[0032] 1) Add water to white cement, talcum powder, lime calcium, cellulose ether, water-resistant rubber powder, bentonite, cellulose, thickener, and defoamer, and stir well to mix evenly.
[0033] 2) After the mixed material is dried by a putty powder dryer, it can be packaged for use.
Embodiment 3
[0035] A kind of waterproof putty powder, in parts by weight, comprises the following components:
[0036] 45 parts of white cement, 40 parts of talcum powder, 35 parts of lime calcium, 2 parts of cellulose ether, 3 parts of water-resistant rubber powder, 12 parts of bentonite, 2 parts of cellulose, 1 part of thickener, and 0.1 part of defoamer.
[0037] Its preparation method comprises the following steps:
[0038] 1) Add water to white cement, talcum powder, lime calcium, cellulose ether, water-resistant rubber powder, bentonite, cellulose, thickener, and defoamer, and stir well to mix evenly.
[0039] 2) After the mixed material is dried by a putty powder dryer, it can be packaged for use.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com