Production process of high-strength marine oil containment boom material
A production process, technology of oil boom
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment Construction
[0059] The following are specific embodiments of the present invention and the accompanying drawings to further describe the technical solutions of the present invention, but the present invention is not limited to these embodiments.
[0060] The production process of the high-strength marine oil boom material includes the following steps:
[0061] S1. Anti-wicking treatment of ordinary polyester yarn, using polyester yarn plain weave fabric with a linear density of 1000D×1000D as the base fabric layer;
[0062] S2. Put 70-90 parts of PVC paste resin, 0.5-1 part of antifungal agent, 5-10 parts of cold-resistant agent, 10-15 parts of titanium dioxide, and 4-8 parts of opacifying agent into the stirring device according to parts by weight and stir evenly , to obtain PVC white paste; in the present embodiment, 74 parts by weight of PVC paste resin, 0.8 part of antifungal agent, 6.2 parts of cold-resistant agent, 13 parts of titanium dioxide, and 6 parts of opacifying agent are pu...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More 