Odorless color asphalt composition and preparation method thereof
A technology of colored asphalt and composition, which is applied in the direction of building structure, building components, building insulation materials, etc., can solve the problems of reducing emissions, achieve the effects of improving workability, improving storage stability, and reducing production and volatilization
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0029] The present invention also provides a method for preparing the above-mentioned odor-cleaning colored asphalt composition, the steps are as follows:
[0030] (1): Add base oil according to the weight percentage ratio, heat to 165°C-175°C, add thermoplastic styrene-butadiene rubber and stir to melt;
[0031] (2) After completely dissolving, add petroleum resin, anti-aging agent, viscosity-increasing additive, odor inhibitor and surfactant in sequence, stir and mix evenly, and develop for 1 hour to prepare the odor-cleaning colored asphalt composition.
Embodiment 1
[0034] Take by weight 40 parts of aromatic hydrocarbon oil, 15 parts of C 9 Petroleum resin, 20 parts of styrene-butylene-styrene segmented copolymer, 1 part of anti-aging agent, 0.5 part of tackifier, 0.5 part of odor inhibitor and 0.8 part of surfactant.
[0035] Heat the aromatic oil to 165°C-175°C, add 20 parts of styrene-butylene-styrene block copolymer and stir to melt;
[0036] After complete dissolution, add 15 parts of C 9 Petroleum resin, 1 part of anti-aging agent, 0.5 part of tackifier, 0.5 part of odor inhibitor and 0.8 part of surfactant. After stirring and mixing evenly, develop for 1 hour, and the clean-odour colored asphalt composition is prepared. See Table 2 for conventional technical indicators for testing colored asphalt.
Embodiment 2
[0038] Take by weight 45 parts of heavy oil minus secondary fission heavy oil, 18 parts of C 9 Petroleum resin, 30 parts of styrene-butylene-styrene block copolymer, 2 parts of anti-aging agent, 0.5 part of tackifier, 1 part of odor inhibitor and 0.5 part of surfactant.
[0039] Heat the heavy oil to 165°C to 175°C, add 30 parts of styrene-butylene-styrene block copolymer and stir to melt the heavy oil;
[0040] After complete dissolution, add 18 parts of C 9 Petroleum resin, 2 parts of anti-aging agent, 1 part of tackifier, 1 part of odor inhibitor and 0.5 part of surfactant. After stirring and mixing evenly, develop for 1 hour, and the clean-odour colored asphalt composition is prepared. See Table 2 for conventional technical indicators for testing colored asphalt.
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com