A kind of ultra-thin glove and preparation method thereof
A glove, ultra-thin technology, applied in gloves, other household appliances, household appliances, etc., can solve the problems of gloves easy to penetrate glue, poor wearing comfort, user irritation, etc., to achieve more comfort and reduce hand fatigue.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0032] Select polyurea coating components, calculated by weight percentage, polyurea 90%, dye 10%.
[0033] By dipping.
[0034] First, heat the polyurea coating compound and maintain the temperature at 80°C, put a glove core on the hand mold, and heat the hand mold so that the temperature of the glove core before dipping is controlled at 50°C; the glove core maintains the above temperature, Dip the glove core into the polyurea coating material at a certain angle for 3 seconds; drip glue on the dipping tank for 1 min; soak the glove core after dipping in 5-10% ethanol aqueous solution for 2 min; at room temperature Let it stand for 20-60 minutes, and the ultra-thin glove product will be obtained after the polyurea coating is completely solidified.
Embodiment 2
[0036] The polyurea coating component is selected, calculated by weight percentage, polyurea 100%.
[0037] By dipping.
[0038] First, heat the polyurea coating rubber and maintain the temperature at 70°C, put a glove core on the hand mold, and heat the hand mold so that the temperature of the glove core before dipping is controlled at 60°C; the glove core maintains the above temperature, Dip the glove core into the polyurea coating rubber at a certain angle for 5 seconds; drip glue on the dipping tank for 2 minutes; soak the glove core after dipping in 5-10% ethanol aqueous solution for 2 minutes; at room temperature Let it stand for 20-60 minutes, and the ultra-thin glove product will be obtained after the polyurea coating is completely solidified.
Embodiment 3
[0040] Select the polyurea coating components, calculated by weight percentage, polyurea 90%, epoxy resin adhesive 10%.
[0041] By dipping.
[0042] First, heat the polyurea coating rubber and maintain the temperature at 60°C, put a glove core on the hand mold, and heat the hand mold so that the temperature of the glove core before dipping is controlled at 60°C; the glove core maintains the above temperature, Dip the glove core into the polyurea coating rubber at a certain angle for 5 seconds; drip glue on the dipping tank for 2 minutes; soak the glove core after dipping in 5-10% ethanol aqueous solution for 2 minutes; at room temperature Let it stand for 20-60 minutes, and the ultra-thin glove product will be obtained after the polyurea coating is completely solidified.