Embodiment 1
[0035] This embodiment provides a sliding vane made of yttria stabilized tetragonal polycrystalline zirconia ceramic material, which can be used in vane compressors. The manufacturing method of the slide is:
[0036] First, a powder mixture containing zirconia and yttrium oxide is prepared and dried. In this embodiment, the ratio (molar percentage) of zirconia powder and yttrium oxide powder used for the sliding sheet is 97% to 98% zirconia, 2% to 3% yttrium oxide. Then the two powders are mixed through a ball mill.
[0037] Then, the powder mixture is sprayed and granulated, and the powder mixture is molded into the shape of a slippery sheet through an appropriate molding process. After removing the grease, the formed sliding piece is heated in a furnace at a certain temperature for a period of time to obtain a sintered sliding piece.
[0038] Finally, the above-mentioned sliding plate is finished to meet the requirements of use.
Embodiment 2
[0040] This embodiment also provides a sliding vane made of yttria stabilized tetragonal polycrystalline zirconia ceramic material, which can be used in vane compressors. The ratio of zirconia powder and yttrium oxide powder in this example is different from that in Example 1. Specifically, the manufacturing method of the slide sheet of this embodiment is:
[0041] First, a powder mixture containing zirconia and yttrium oxide is prepared and dried. In this embodiment, the ratio (mol %) of zirconia powder and yttrium oxide powder used for the sliding plate is 91% to 93% zirconia and 7% to 9% yttrium oxide. Then the two powders are mixed through a ball mill.
[0042] Then, the powder mixture is sprayed and granulated, and the powder mixture is molded into the shape of a slippery sheet through an appropriate molding process. After removing the grease, the formed sliding piece is heated in a furnace at a certain temperature for a period of time to obtain a sintered sliding piece.
[...
Embodiment 3
[0051] This embodiment provides a sliding vane made of cerium oxide stabilized tetragonal polycrystalline zirconia toughened ceramic material, and the sliding vane can be used in a sliding vane compressor. The manufacturing method of the slide is:
[0052] First, a powder mixture containing zirconia and cerium oxide is prepared and dried. In this embodiment, the ratio (molar percentage) of the zirconia powder and the cerium oxide powder used for the sliding sheet is: 85% to 88% zirconia and 12% to 15% cerium oxide. The two powders are mixed through a ball mill.
[0053] Then, the powder mixture is sprayed and granulated, and the powder mixture is molded into the shape of a slippery sheet through an appropriate molding process. After removing the grease, the formed sliding piece is heated in a furnace at a certain temperature for a period of time to obtain a sintered sliding piece.
[0054] Finally, the above-mentioned sliding plate is finished to meet the requirements of use.
PUM
| Property | Measurement | Unit |
|---|---|---|
| particle size | aaaaa | aaaaa |
| hardness | aaaaa | aaaaa |
| density | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More 