Fluorescent wristband for intelligent bracelet and preparation method thereof
A smart wristband and fluorescent technology, applied in the direction of watch straps, chemical instruments and methods, applications, etc., can solve problems such as wear, wristband wear resistance and insufficient mechanical properties
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0013] The invention provides a method for preparing a fluorescent wristband for smart bracelets, the preparation method comprising:
[0014] (1) Polyethylene, polypropylene, nylon fiber, polycarbonate, attapulgite, phenolic resin, vinyl tri-tert-butylperoxysilane, ethylene bisstearamide, plasticizer and anti-aging agent are mixed. After thermoplastic molding and shearing, a sheet-shaped green body is obtained;
[0015] (2) The fluorescent material is mixed between two sheet-shaped green bodies, and the master batch is obtained after hot pressing; the fluorescent material is composed of strontium aluminate, phosphate ammonium and ethylene glycol in a mass ratio of 1:0.4-0.5:0.2 The ratio of -0.4 is mixed to obtain;
[0016] (3) Extrude the masterbatch to obtain a fluorescent wristband; wherein, the extrusion molding conditions at least include: the temperature of the machine head is 65-70°C, the temperature of the extrusion section of the barrel is 50-55°C, the machine The t...
Embodiment 1
[0026] Mix polyethylene, polypropylene, nylon fiber, polycarbonate, attapulgite, phenolic resin, vinyl tri-tert-butylperoxysilane, ethylene bisstearamide, dioctyl phthalate and antioxidant 4010NA , after thermoplastic molding and shearing, a sheet-shaped green body was obtained; the fluorescent material was mixed between two sheet-shaped green bodies, and the masterbatch was obtained after hot pressing (at a temperature of 70°C and a time of 1 min); the fluorescent material It is obtained by mixing strontium aluminate, ammonium phosphate and ethylene glycol according to the mass ratio of 1:0.4:0.2; the masterbatch is extruded to obtain a fluorescent wristband; wherein, the extrusion molding conditions include at least: machine head The temperature of the barrel is 65°C, the temperature of the extrusion section of the barrel is 50°C, the temperature of the plasticizing section of the barrel is 70°C, and the temperature of the screw is 50°C. Relative to 100g of polyethylene, the...
Embodiment 2
[0028] Mix polyethylene, polypropylene, nylon fiber, polycarbonate, attapulgite, phenolic resin, vinyl tri-tert-butylperoxysilane, ethylene bisstearamide, butyl benzyl phthalate and antioxidant RD , after thermoplastic molding and shearing, a sheet-shaped green body was obtained; the fluorescent material was mixed between two sheet-shaped green bodies, and the master batch was obtained after hot pressing (at a temperature of 80°C and a time of 3 minutes); the fluorescent material It is obtained by mixing strontium aluminate, amine phosphate and ethylene glycol according to a mass ratio of 1:0.5:0.4; extruding the masterbatch to obtain a fluorescent wristband; wherein, the extrusion molding conditions include at least: machine head The temperature of the barrel is 70°C, the temperature of the extrusion section of the barrel is 55°C, the temperature of the plasticizing section of the barrel is 75°C, and the temperature of the screw is 55°C. Relative to 100g of polyethylene, the ...