[0013] A dye suitable for willow weaving is prepared by the following components in parts by weight: 35 parts of disperse dyes, 10 parts of cinnamaldehyde derivative modified polyvinyl alcohol, 3 parts of glycerin, 3 parts of diethanolamine, 5 parts of nanometer calcium carbonate, 2 parts of α-olefin sulfonate, 0.5 parts of sodium phosphate, 1.6 parts of sodium dihydrogen phosphate, 100 parts of water, and 30 parts of 1,4-butanediol.
[0014] Further, the preparation method of the cinnamaldehyde derivative modified polyvinyl alcohol comprises the following steps:
[0015] Cinnamaldehyde derivatives were mixed with deionized water to prepare a cinnamaldehyde derivative solution with a mass fraction of 3.2%, and then 0.015% of its mass polyacetamide was added to the cinnamaldehyde derivative solution, followed by ultrasonic treatment for 5 minutes to obtain a modified Mix the polyvinyl alcohol and the modified liquid uniformly at a volume ratio of 20:1.3, stir at 1200r / min for 5...
Embodiment 2
[0021] A dye suitable for willow weaving is prepared by the following components in parts by weight: 35 parts of disperse dyes, 12 parts of cinnamaldehyde derivative modified polyvinyl alcohol, 3 parts of glycerin, 3 parts of diethanolamine, 5 parts of nanometer calcium carbonate, 2 parts of α-olefin sulfonate, 0.5 parts of sodium phosphate, 1.6 parts of sodium dihydrogen phosphate, 100 parts of water, and 30 parts of 1,4-butanediol.
[0022] Further, the preparation method of the cinnamaldehyde derivative modified polyvinyl alcohol comprises the following steps:
[0023] Cinnamaldehyde derivatives were mixed with deionized water to prepare a cinnamaldehyde derivative solution with a mass fraction of 3.2%, and then 0.015% of its mass polyacetamide was added to the cinnamaldehyde derivative solution, followed by ultrasonic treatment for 5 minutes to obtain a modified Mix the polyvinyl alcohol and the modified liquid uniformly at a volume ratio of 20:1.3, stir at 1200r / min for 5...
Embodiment 3
[0029] A dye suitable for willow weaving is prepared by the following components in parts by weight: 35 parts of disperse dyes, 11 parts of cinnamaldehyde derivative modified polyvinyl alcohol, 3 parts of glycerin, 3 parts of diethanolamine, 5 parts of nanometer calcium carbonate, 2 parts of α-olefin sulfonate, 0.5 parts of sodium phosphate, 1.6 parts of sodium dihydrogen phosphate, 100 parts of water, and 30 parts of 1,4-butanediol.
[0030] Further, the preparation method of the cinnamaldehyde derivative modified polyvinyl alcohol comprises the following steps:
[0031] Cinnamaldehyde derivatives were mixed with deionized water to prepare a cinnamaldehyde derivative solution with a mass fraction of 3.2%, and then 0.015% of its mass polyacetamide was added to the cinnamaldehyde derivative solution, followed by ultrasonic treatment for 5 minutes to obtain a modified Mix the polyvinyl alcohol and the modified liquid uniformly at a volume ratio of 20:1.3, stir at 1200r / min for 5...
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com