A technology of energy saving, environmental protection and manufacturing method, applied in the field of porcelain manufacturing, can solve the problems of low thermal stability and strength, affecting practicability, environmental pollution, etc., and achieve the effect of good function, healthy production process and exquisite pattern
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0029] A method for manufacturing energy-saving and environment-friendly daily art porcelain, which comprises the following steps:
[0030] Step 1: Prepare the Slime
[0031] 1.1) Select and crush all the raw materials used for the blank, bottom glaze and surface glaze and pass through a 20-mesh sieve for later use;
[0032] 1.2) Weigh the raw materials of blank, bottom glaze and surface glaze according to the corresponding formula, add water and ball mill for a corresponding time, and then obtain mud, bottom glaze slurry and surface glaze slurry respectively;
[0033] 1.3) Pass the mud obtained in step 1.2) through a 220-mesh sieve, remove iron and press filter to obtain a 21%-25% mud cake, then vacuum mud for 3 times, and keep it stale for 5-7 days and seal it for later use; Step 1.2) Pass the bottom glaze slurry through a 220-mesh sieve, pass the top glaze slurry through a 250-mesh sieve, and remove iron through a magnetic separator to obtain a bottom glaze with a concentr...
Embodiment 2
[0045] A method for manufacturing energy-saving and environment-friendly daily art porcelain, which comprises the following steps:
[0046] Step 1: Prepare the Slime
[0047] 1.1) Select and crush all the raw materials used for the blank, bottom glaze and surface glaze and pass through a 20-mesh sieve for later use;
[0048] 1.2) Weigh the raw materials of blank, bottom glaze and surface glaze according to the corresponding formula, add water and ball mill for a corresponding time, and then obtain mud, bottom glaze slurry and surface glaze slurry respectively;
[0049] 1.3) Pass the mud obtained in step 1.2) through a 220-mesh sieve, remove iron and press filter to obtain a 21%-25% mud cake, then vacuum mud for 3 times, and keep it stale for 5-7 days and seal it for later use; Step 1.2) Pass the bottom glaze slurry through a 220-mesh sieve, pass the top glaze slurry through a 250-mesh sieve, and remove iron through a magnetic separator to obtain a bottom glaze with a concentr...