Asphalt mixture vibrating mixing indoor test operation method and device

A technology for asphalt mixture and indoor testing, which is used in measuring devices, material inspection products, analytical materials, etc., to achieve the effect of extending service life, improving road performance and facilitating promotion

Active Publication Date: 2019-02-15
CHANGSHA UNIVERSITY OF SCIENCE AND TECHNOLOGY
View PDF10 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0008] The purpose of the present invention is to provide a vibratory mixing indoor test device for asphalt mixture, which solves the problem of "agglomerates" of fine aggregates and fillers in asphalt mixture, and overcomes the friction and viscous force between the aggregated material particles

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Asphalt mixture vibrating mixing indoor test operation method and device
  • Asphalt mixture vibrating mixing indoor test operation method and device
  • Asphalt mixture vibrating mixing indoor test operation method and device

Examples

Experimental program
Comparison scheme
Effect test

Embodiment

[0045] The comparison between conventional non-vibration mixing and vibrating mixing of asphalt mixture indoor test device:

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

PropertyMeasurementUnit
eccentricityaaaaaaaaaa
Login to view more

Abstract

The invention discloses an asphalt mixture vibrating mixing indoor test operation method and an asphalt mixture vibrating mixing indoor test device. The asphalt mixture vibrating mixing indoor test device consists of a mixing tank, a machine frame, a mixing tank vibrator, a vibration-absorbing device, a stirring motor, stirring shafts, stirring arms, stirring blades, a shaft end sealing device, avibrating motor, a vibration exciter, a material quantity detecting device, a heating device, a heater, an electrical control system, a control panel and a discharge door. By the operation method of the asphalt mixture vibrating mixing indoor test device, simultaneous heating of the mixing tank and the stirring shafts is achieved, the vibrating frequency of the mixing tank and shaft bodies can becontrolled, the vibrating amplitudes can be controlled, and the discharge amount can be controlled. The asphalt mixture vibrating mixing indoor test device is convenient to operate and easy to popularize and apply; each material component is redispersed uniformly, the void ratio is reduced, and the mixing quality of a mixture is improved; and the asphalt mixture vibrating mixing indoor test deviceis of a great significance in stimulating the potential of materials, improving the road performance of an asphalt pavement and prolonging the service life of the asphalt pavement.

Description

technical field [0001] The invention belongs to the technical field of road engineering, and relates to an indoor test operation method and device for asphalt mixture vibration mixing. Background technique [0002] With the development of road construction and research in our country, according to relevant highway statistics and construction experience in various places, the main problem of asphalt pavement is the gradual damage of the road surface caused by local damage, which is often one or two years after the pavement is completed. Early failure in years or years in the form of cracks, water damage, loosening, potholes, and excessive car removal. Early failure of asphalt pavement has always been a major problem in the engineering field. The inhomogeneity of asphalt mixture is the main cause of early failure of asphalt pavement. The degree of uniformity of asphalt mixture is directly related to the mechanical properties and service life of asphalt pavement. [0003] Asph...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): G01N33/42G01N1/44G01N1/38
CPCG01N1/38G01N1/44G01N33/42G01N2001/386
Inventor 郑健龙张良奇张军辉刘韡堃李冠峰黄拓孔鲜宁李鹏
Owner CHANGSHA UNIVERSITY OF SCIENCE AND TECHNOLOGY
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products