A hydrophilic silicone oil and preparation technology, which is applied in fiber treatment, textiles and papermaking, etc., can solve the problems of insufficient smoothness of the cloth surface and reduced comfort, and achieve the effects of good smoothness, avoiding yellowing, and strong hydrophilicity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0055] A kind of hydrophilic silicone oil finishing agent, comprising the first silicone oil auxiliary agent, the second silicone oil auxiliary agent, 25 parts of parabens and 60 parts of softening agent, the first silicone oil auxiliary agent comprises the following components in parts by weight: hydrophilic amino group 50 parts of silicone oil, 32 parts of polydimethylsiloxanol beswaxate, 6 parts of disodium dicarboxyethyl cocoyl propylenediamine and 90 parts of ethylene glycol monobutyl ether. The second silicone oil additive includes the following components in parts by weight: 60 parts of terpolymerized block silicone oil, 14 parts of disodium dicarboxyethylcocoylpropylenediamine, and 90 parts of ethylene glycol monobutyl ether.
Embodiment 2
[0056] Embodiment 2: The difference from Example 1 is that the first silicone oil auxiliary agent includes the following components in parts by weight: 50 parts of hydrophilic amino silicone oil, 32 parts of polydimethylsiloxanol meswaxate, dicarboxyethyl 6 parts of cocoyl propylene diamine disodium, 90 parts of ethylene glycol monobutyl ether and 15 parts of nano-oxidized polyethylene wax emulsion.
[0057] refer to figure 1 A preparation process for the hydrophilic silicone oil finishing agent in Preparation Example 2 comprises the following steps:
[0058] S1: configuring the first silicone oil additive, including the following steps:
[0059] a: Add ethylene glycol monobutyl ether into the first reaction kettle first.
[0060] b: Adjust the temperature in the first reactor to which ethylene glycol monobutyl ether is added to 25°C, and keep the temperature in the first reactor at 25°C. Then add the hydrophilic amino silicone oil into the first reaction kettle, stir while...