Clear water dyeing emulsion and preparation method thereof
An emulsion and water technology, applied in pharmaceutical formulations, cosmetic preparations, cosmetic preparations, etc., can solve problems such as scalp damage and achieve a healthy and shiny effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0057] The present invention also provides a method for preparing a clear water dye emulsion, which is characterized in that it includes a dye preparation method,
[0058] The steps are as follows:
[0059] 1) Dissolve propylene glycol, acrylate copolymer, sodium sulfite, and disodium EDTA in water and heat to dissolve it, and keep it at 80℃-85℃ for 20 minutes;
[0060] 2) Cool with a cooling water jacket, add colorants, antioxidants, tea extract, and ginseng extract after reaching 60°C, cool with a cooling water jacket, and cool to below 45°C;
[0061] 3) Add ammonium hydroxide and flavor, mix well and take samples for inspection, discharge and fill after passing the test.
[0062] The present invention further provides: a preparation method of a clear water dye emulsion, the plant extract includes tea extract and ginseng root extract.
[0063] The present invention further provides: a preparation method of a clear water dye emulsion, including a preparation method of an oxidizing agent...
Embodiment 1
[0069] In this embodiment, a clear water dye emulsion includes a dye and an oxidizer, and the dye includes the following components by weight percentage:
[0070]
[0071] The oxidant includes the following components by weight percentage:
[0072]
[0073]
[0074] The present invention further provides that the plant extract includes tea extract and ginseng root extract, and the weight percentage content of the two is: tea extract 0.1% and ginseng root extract 0.1%.
[0075] The preparation method is as follows: including the preparation method of the dye, the steps are as follows:
[0076] 1) Dissolve propylene glycol, acrylate copolymer, sodium sulfite, and disodium EDTA in water and heat to dissolve it, and keep it at 80℃-85℃ for 20 minutes;
[0077] 2) Cool with a cooling water jacket, add colorants, antioxidants, tea extract, and ginseng extract after reaching 60°C, cool with a cooling water jacket, and cool to below 45°C;
Embodiment 2
[0085] The difference between this embodiment and Embodiment 1 lies in the content of plant extracts: the weight percentage content of plant extracts in this embodiment is 0.4%, of which tea extract is 0.2% and ginseng root extract is 0.2%.