Embodiment 1
[0048] A bright red card made of the following raw materials: 20% needle leaves, 60% broadleaf, and 20% waste paper.
[0049] A method for making a bright red card, comprising the following steps:
[0050] A. Pulping preparation
[0051] 1) wood pulp pulping: put the wood pulp board into the hydropulper, and disintegrate it by the hydropulper;
[0052] 2) Wood pulp refining: the crushed pulp is refined through a double-disk refiner, and the fibers are kneaded and extruded by the toothed discs in the grinding zone to complete the beating process to form pulp;
[0053] Wood pulp beating degree: 35°SR, wet weight of softwood pulp: 6g, wet weight of hardwood pulp: 1.6g;
[0054] 3) Waste paper pulping: In order to reduce production costs, some waste paper pulp is used.
[0055] Waste paper pulping process: Firstly, it goes through a hydropulper, hydropulper → fiber separator (re-shredding and separation) → sand remover (removal of impurities) → pressure screen (removal of coars...
Embodiment 2
[0084] A bright red card made of the following raw materials: needle leaves 30%, broadleaf 55%, waste paper 15%.
[0085] A method for making a bright red card, comprising the following steps:
[0086] A. Pulping preparation
[0087] 1) wood pulp pulping: put the wood pulp board into the hydropulper, and disintegrate it by the hydropulper;
[0088] 2) Wood pulp refining: the crushed pulp is refined through a double-disc refiner, and the fibers are kneaded and extruded by the toothed discs in the grinding zone to complete the beating process to form pulp;
[0089] Wood pulp beating degree: 38°SR, wet weight of softwood pulp: 7g, wet weight of hardwood pulp: 2.2g;
[0090] 3) Waste paper pulping: In order to reduce production costs, some waste paper pulp is used.
[0091] Waste paper pulping process: Firstly, it goes through a hydropulper, hydropulper → fiber separator (re-shredding and separation) → sand remover (removal of impurities) → pressure screen (removal of coarse im...
Embodiment 3
[0120] A bright red card made of the following raw materials: needle leaves 25%, broadleaf 58%, waste paper 12%.
[0121] A method for making a bright red card, comprising the following steps:
[0122] A. Pulping preparation
[0123] 1) wood pulp pulping: put the wood pulp board into the hydropulper, and disintegrate it by the hydropulper;
[0124] 2) Wood pulp refining: the crushed pulp is refined through a double-disk refiner, and the fibers are kneaded and extruded by the toothed discs in the grinding zone to complete the beating process to form pulp;
[0125] Wood pulp beating degree: 35-42°SR, wet weight of softwood pulp: 6-7g, wet weight of hardwood pulp: 1.6-2.2g;
[0126]3) Waste paper pulping: In order to reduce production costs, some waste paper pulp is used.
[0127] Waste paper pulping process: Firstly, it goes through a hydropulper, hydropulper → fiber separator (re-shredding and separation) → sand remover (removal of impurities) → pressure screen (removal of c...
PUM
Property | Measurement | Unit |
---|---|---|
diameter | aaaaa | aaaaa |
diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com